# US 4,395,340 A · Enhanced oil recovery methods and systems

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,395,340 A
- Document ID: US4395340A
- Status: Granted
- Kind: A
- Application number: 06/282,989
- Filed: 1981-07-14
- Granted: 1983-07-26
- Earliest claimed: 1981-07-14
- Assignees: Halliburton Company
- Inventors: Homer C. McLaughlin
- Web page: https://patentgrep.com/patent/US4395340A

## CPC

- C08F 2/10: Aqueous solvent
- C09K 8/588: characterised by the use of specific polymers {(polymeric surfactants C09K8/584)}
- Y10S 507/936: Flooding the formation
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method of enhanced oil recovery from subterranean oil-containing formations via injection through an injection well penetrating the formation of a viscous aqueous solution containing one or more water-soluble organic polymers and forcing such solution through the formation towards a production well for ultimate recovery. The viscous aqueous polymer solutions of the invention are prepared at the site of their use by polymerizing one or more water-soluble polymerizable vinyl monomers in aqueous solutions which may contain high concentrations of one or more salts.

## Claims

### Claim 1

A method of enhancing the recovery of oil from a subterranean oil-containing formation comprising injecting a viscous aqueous solution containing one or more water-soluble organic polymers into the formation by way of at least one injection well penetrating the formation and forced through the formation towards at least one production well penetrating the formation, and further comprising
combining water-soluble polymerizable vinyl monomers and a water-soluble ionizing sulfite with an aqueous inorganic salt solution at the site of said injection and production wells whereby said monomers are rapidly polymerized to form a concentrated high viscosity polymer solution, said water-soluble polymerizable vinyl monomers being selected from the group consisting of acrylamide monomers alone, and acrylamide monomers and one or more other vinyl monomers which are copolymerizable therewith;
diluting said concentrated high viscosity polymer solution with additional aqueous fluid at the site of said injection and production wells to form an injection solution having a desired viscosity; and
injecting said injection solution into said formation.

### Claim 2 (depends on 1)

The method of claim 1 which is further characterized to include the step of combining a buffer with said aqueous inorganic salt solution in a quantity sufficient to maintain the pH thereof at about 7 prior to combining said monomers and said sodium sulfite with said solution.

### Claim 3 (depends on 2)

The method of claim 2 wherein said water-soluble ionizing sulfite is selected from the group consisting of alkaline metals, ammonium and substituted ammonium sulfites, bisulfites, pyrosulfites, metabisulfites, and mixtures thereof.

### Claim 4 (depends on 2)

The method of claim 2 wherein said water-soluble ionizing sulfite is sodium sulfite.

### Claim 5 (depends on 1)

The method of claim 1 wherein said aqueous inorganic salt solution contains one or more salts selected from the group consisting of alkali metal salts of strong inorganic acids.

### Claim 6 (depends on 1)

The method of claim 1 wherein said water-soluble polymerizable vinyl monomers are acrylamide monomers alone and the polymer formed is polyacrylamide.

### Claim 7 (depends on 1)

The method of claim 1 wherein said water-soluble polymerizable vinyl monomers are acrylamide monomers and acrylic acid monomers and the polymer formed is a copolymer of acrylamide and and a salt of acrylic acid.

### Claim 8 (depends on 5)

The method of claim 5 wherein said aqueous inorganic salt solution contains one or more of said salts in a concentration of at least about 12% by weight of said solution.

### Claim 9 (depends on 8)

The method of claim 8 wherein said water-soluble polymerizable vinyl monomers are combined with said aqueous salt solution in an amount in the range of from about 1% to about 10% by weight of the resulting aqueous monomer-salt solution.

### Claim 10 (depends on 9)

The method of claim 9 wherein said water-soluble ionizing sulfite is combined with said aqueous monomer-salt solution in an amount in the range of from about 0.001% to about 0.1% by weight of the resulting aqueous sulfite-monomer-salt solution.