# US 4,394,433 A · Diazonium imaging system

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,394,433 A
- Document ID: US4394433A
- Status: Granted
- Kind: A
- Application number: 06/286,197
- Filed: 1981-07-23
- Granted: 1983-07-19
- Earliest claimed: 1979-12-07
- Assignees: Minnesota Mining and Manufacturing Company
- Inventors: Kenneth G. Gatzke
- Web page: https://patentgrep.com/patent/US4394433A

## CPC

- G03C 1/732: {Leuco dyes}
- G03C 1/61: with non-macromolecular additives
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)

## Abstract

A novel light sensitive, heat developable imaging system incorporating a diazonium salt and a leuco dye in a binder is disclosed.

## Claims

### Claim 1

An article comprising a light sensitive, positive-acting, heat developable, dry layer on a substrate, the dry ingredients of said layer comprising at least 25% by weight of a polymeric binder, at least 0.3% by weight of a leuco dye capable of being oxidized to a colored form upon only heating, a sufficient amount of a photosensitive diazonium salt to oxidize said leuco dye to a colored form in non-light struck portions of said layer, and less than 0.1 mole nitrate ion per 1.0 mole leuco dye, said leuco dye in said layer being present in a concentration sufficient to provide an increase in optical density upon development of at least 0.2.

### Claim 2 (depends on 1)

The article of claim 1 wherein said leuco dye in said layer is present as at least 1% by weight of dry ingredients of said layer.

### Claim 3 (depends on 1)

The article of claim 1 wherein said leuco dye in said layer is present in the amount of 2% to 10% by weight of dry ingredients of said layer.

### Claim 4 (depends on 1)

The article of claim 1 wherein said leuco dye in said layer is present in a concentration sufficient to provide an increase in optical density upon development of at least 0.6.

### Claim 5 (depends on 1)

The article of claim 1 wherein said leuco dye in said layer is present in a concentration sufficient to provide an increase in optical density upon development of at least 1.0.

### Claim 6 (depends on 1)

The article of claim 1 wherein said leuco dye in said layer is selected from the class consisting of leuco crystal violet and leuco malechite green.

### Claim 7 (depends on 1)

The article according to claim 1 wherein said layer comprises the diazonium salt 1-diazo-2,5-diethoxy-4-morpholino benzene borofluoride.

### Claim 8 (depends on 1)

The article according to claim 1 wherein the development temperature of said layer is between 180.degree. F. (82.degree. C.) and 380.degree. F. (193.degree. C.).

### Claim 9 (depends on 1)

The article according to claim 1 wherein the development temperature of said layer is between 220.degree. F. (105.degree. C.) and 350.degree. F. (167.degree. C.).

### Claim 10 (depends on 1)

The article according to claim 1 wherein said binder in said layer is selected from the class consisting of polyvinyl chloride and polyvinyl acetate resins.

### Claim 11 (depends on 10)

The article according to claim 10 wherein said binder in said layer is present as at least 25% by weight of dry ingredients in the layer.

### Claim 12 (depends on 10)

The article according to claim 10 wherein said binder in said layer is present as at least 50% by weight of dry ingredients in the layer.

### Claim 13 (depends on 10)

The article according to claim 10 wherein said binder in said layer is present as at least 70% by weight of dry ingredients in the layer.

### Claim 14

An article comprising a light sensitive, positive-acting, heat developable, dry layer on a substrate, the dry ingredients of said layer consisting essentially of at least 25% by weight of a polymeric binder, at least 0.3% by weight of a leuco dye capable of being oxidized upon only heating to a colored form, a sufficient amount of a photosensitive diazonium salt to oxidize said leuco dye to a colored form in non-light struck portions of said layer, and less than 0.1 mole nitrate ion per 1.0 mole leuco dye, said leuco dye in said layer being present in a concentration sufficient to provide an increase in optical density upon development of at least 0.2.

### Claim 15 (depends on 14)

The article according to claim 14 wherein said layer further consists of an amount of phenidone sufficient to depress the Dmin value of said layer.

### Claim 16

An article comprising a light sensitive, positive-acting, heat developable, dry layer on a substrate, the dry ingredients of said layer consisting of at least 25% by weight of a polymeric binder, at least 0.3% by weight of a leuco dye capable of being oxidized upon only heating to a colored form, a sufficient amount of a photo-sensitive diazonium salt to oxidize said leuco dye to a colored form in non-light struck portions of said layer, and less than 0.1 mole nitrate ion per 1.0 mole leuco dye, said leuco dye in said layer being present in a concentration sufficient to provide an increase in optical density upon development of at least 0.2.

### Claim 17

An article comprising a light sensitive, positive-acting, heat developable, dry layer on a substrate, the dry ingredients of said layer consisting of at least 25% by weight of a polymeric binder, at least 0.3% by weight of a leuco dye capable of being oxidized upon only heating to a colored form, a sufficient amount of a photosensitive diazonium salt to oxidize said leuco dye to a colored form in non-light struck portions of said layer, a chemically effective amount of at least one additive selected from antioxidants, complexors, plasticizers, polyketones, stabilizers, surfactants, antistatic agents, coating aids, inhibitors, lubricants, flexibilizers, and fillers, and less than 0.1 mole nitrate ion per 1.0 mole leuco dye, said leuco dye in said layer being present in a concentration sufficient to provide an increase in optical density upon development of at least 0.2.

### Claim 18

A process for imaging an article comprising a light sensitive, positive-acting, heat developable, dry layer on a substrate, the dry ingredients of said layer comprising at least 25% by weight of a polymeric binder, at least 0.3% by weight of a leuco dye capable of being oxidized to a colored form upon only heating, a sufficient amount of a photosensitive diazonium salt to oxidize said leuco dye to a colored form in non-light struck portions of said layer, and less than 0.1 mole nitrate ion per 1.0 mole leuco dye, said leuco dye in said layer being present in a concentration sufficient to provide an increase in optical density upon development of at least 0.2, said process comprising the steps: a. exposing said article to an image-wise distribution of radiation to destroy said diazonium salt in light-struck areas, and
b. heating said article to enable said diazonium salt to oxidize said leuco dye to a colored form in non light-struck areas to produce said positive image.