# US 4,392,925 A · Electrode arrangement in a cell for manufacture of aluminum from molten salts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,392,925 A
- Document ID: US4392925A
- Status: Granted
- Kind: A
- Application number: 06/257,891
- Filed: 1981-04-27
- Granted: 1983-07-12
- Earliest claimed: 1980-05-14
- Assignees: Swiss Aluminium Ltd.
- Inventors: Hanspeter Alder; Eugen Schalch
- Web page: https://patentgrep.com/patent/US4392925A

## CPC

- C25C 3/08: Cell construction, e.g. bottoms, walls, cathodes
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR

## Abstract

The durability of oxide-ceramic anodes can be increased, if the aluminum surface which lies opposite the active anode surface and is in direct contact with the molten electrolyte, is smaller than the active anode surface. The separated aluminum is collected on the floor of the carbon lining and is sub-divided by an insulating material into pools, which are connected together by means of tubes or channels. The total of all the aluminum surfaces exposed to the melt amounts to 10-90% of the active anode surface.

## Claims

### Claim 1

An electrolytic cell for use in the production of aluminum comprising:
a pot having a floor and sidewalls;
a melt of liquid aluminum within said pot on said floor;
a molten electrolyte within said pot on said melt of liquid aluminum;
at least one anode within said pot projecting into said molten electrolyte such that the top surface of said melt of liquid aluminum is a distance d from the active bottom surface of said at least one anode; and
insulating means within said pot in said melt of liquid aluminum for reducing the surface area of said melt of liquid aluminum in direct contact with said molten electrolyte such that the total surface area of said melt of liquid aluminum exposed to said molten electrolyte is from about 10-90% the active surface area of said at least one anode.

### Claim 2 (depends on 1)

An electrolytic cell according to claim 1 wherein said insulating means for reducing the surface area of said melt of liquid aluminum comprises a plurality of insulated members.

### Claim 3 (depends on 2)

An electrolytic cell according to claim 2 wherein at least one of said plurality of insulated members is provided with a passage for communicating said melt of liquid aluminum.

### Claim 4 (depends on 2)

An electrolytic cell according to claim 2 wherein a plurality of anodes project into said molten electrolyte.

### Claim 5 (depends on 4)

An electrolytic cell according to claim 4 wherein the edges of the active surface area of the anodes lie above said insulated members.

### Claim 6 (depends on 5)

An electrolytic cell according to claim 5 wherein said edges are bevelled concavely.

### Claim 7 (depends on 1)

An electrolytic cell according to claim 1 wherein said at least one anode is a dimensionally stable anode.

### Claim 8 (depends on 1)

An electrolytic cell according to claim 1 wherein said total surface area of said melt of liquid aluminum exposed to said molten electrolyte is from about 20-50% the active surface area of said at least one anode.

### Claim 9 (depends on 1)

An electrolytic cell according to claim 1 wherein at least a portion of said total surface area of said melt of liquid aluminum comprises a wettable cathode body having a film of aluminum deposited thereon.

### Claim 10 (depends on 9)

An electrolytic cell according to claim 9 wherein said wettable cathode body is provided with a passage for communicating said film of aluminum with said melt of liquid aluminum collected on said floor of said pot.

### Claim 11 (depends on 10)

An electrolytic cell according to claim 10 wherein the surface of said melt of liquid aluminum collected on said floor of said pot is at a distance equal to at least 1.5 d from the active surface of said at least one anode.

### Claim 12 (depends on 1)

An electrolytic cell according to claim 1 wherein a plurality of anodes project into said molten electrolyte.

### Claim 13 (depends on 12)

An electrolytic cell according to claim 12 wherein the anodes proximate to said sidewalls of said pot are from about 15-30% narrower than the other anodes.

### Claim 14 (depends on 12)

An electrolytic cell according to claim 12 wherein a plurality of cathode elements are provided within said pot and are arranged alternately with and parallel to said plurality of anodes.

### Claim 15 (depends on 14)

An electrolytic cell according to claim 14 wherein said anodes and said cathodes not proximate to said sidewalls of said pot carry current on both sides.

### Claim 16 (depends on 14)

An electrolytic cell according to claim 14 wherein said anodes and said cathodes are arranged vertically.

### Claim 17 (depends on 12)

An electrolytic cell according to claim 12 wherein said anodes are plate-shaped.

### Claim 18 (depends on 1)

An electrolytic cell according to claim 1 wherein said melt of liquid aluminum is in fluid communication with at least one collection tank.

### Claim 19

A method of improving the stability of an anode used in the electrolysis of aluminum comprising:
providing an electrolytic cell comprising a pot having a floor and sidewalls, a melt of liquid aluminum on said floor and molten electrolyte on said melt of liquid aluminum;
positioning at least one anode within said pot in said molten electrolyte such that the active surface of said at least one anode is a distance d from the top surface of said melt of liquid aluminum; and
providing insulating means in said melt of liquid aluminum for reducing the surface area of said melt of liquid aluminum in direct contact with said molten electrolyte such that the total surface area of said melt of liquid aluminum exposed to said molten electrolyte is from about 10-90% the active surface area of said at least one anode.

### Claim 20 (depends on 19)

A method according to claim 19 including providing a plurality of insulated members for reducing said surface area of said melt of liquid aluminum.

### Claim 21 (depends on 20)

A method according to claim 20 including providing a passage in at least one of said insulated members for communicating said melt of liquid aluminum.

### Claim 22 (depends on 19)

A method according to claim 19 further including providing a wettable cathode body in said melt of liquid aluminum having a film of aluminum deposited thereon.

### Claim 23 (depends on 22)

A method according to claim 22 including providing a passage in said wettable carbon body for communicating said film of aluminum with said melt of liquid aluminum collected on said floor of said pot.

### Claim 24 (depends on 23)

A method according to claim 23 including positioning said melt of liquid aluminum collected on said floor of said pot such that the surface of said melt of said liquid aluminum is at a distance equal to at least 1.5 d from the active surface of said at least one anode.

### Claim 25 (depends on 19)

A method according to claim 19 including providing a plurality of anodes.

### Claim 26 (depends on 25)

A method according to claim 25 including providing a plurality of cathode elements arranged alternately with and parallel to said plurality of anodes.

### Claim 27 (depends on 26)

A method according to claim 26 including arranging said cathodes and said anodes vertically.

### Claim 28 (depends on 19)

A method according to claim 19 including providing at least one collection tank and communicating said melt of liquid aluminum with said at least one collection tank.