Abstract
An improved process for treating coal tar pitch to form anisotropic carbon comprising treating coal tar pitch with picric acid, recovering the resulting picrates, decomposing the picrates and heating the resulting aromatic hydrocarbons to obtain anisotropic carbon in less time.
Claims2
A process for the preparation of anistropic carbon comprising extracting coal tar pitch with an organic solvent, adding picric acid to the extract solution to form picrates, recovering the picrates, decomposing the picrates and heating the resulting coal tar pitch fraction at 350.degree. to 550.degree. C. at a pressure of 0.1 to 50 bar for about 100 to 30 minutes to transform it substantially quantitatively into anisotropic carbon and recovering the anisotropic carbon formed at 350.degree. to 550.degree. C.
Dependencies are inferred from the claim text.