Toughened polyamide flame retarded with octabromodiphenyl ether
AssigneeE. I. Du Pont de Nemours and Company
InventorPaul N. Richardson
Life of this patent
Estimating the term…
Abstract
Toughened flame retardant polyamide molding blend containing a selected octabromodiphenyl ether and a polymeric toughening agent.
Claims3
A toughened, flame-retardant polyamide molding blend consisting essentially of:
- (A) a film-forming polyamide selected from
- (i) poly(hexamethylene adipamide) or,
- (ii) a copolymer of hexamethylene adipamide and caprolactam.
- (B) at least 13% by weight of (A), (B) and (C) of a toughening system containing at least 7% by weight of (A), (B) and (C) of an adduct of (a) an ethylenically unsaturated compound containing carboxyl groups or carboxyl derivatives, and (b) a copolymer of ethylene, at least one C.sub.3 to C.sub.6 .alpha.-olefin, and at least one nonconjugated diene, said unsaturated compound being present in the adduct in an amount such that the anhydride functionality is at least 0.05 meq/g of adduct, and 0-8% of (A), (B) and (C) of a toughening extender;
- and
- (C) at least 24% by weight of (A), (B) and (C) of a flame retardant system composed of
- (i) at least 17% by weight of (A), (B) and (C) of octabromodiphenyl ether, and
- (ii) antimony trioxide present in an amount of at least 5.9% by weight of (A), (B) and (C).
5 more elements
Dependencies are inferred from the claim text.