Reductants for reducing metals in acid media
AssigneeUranium Recovery Corporation
InventorsRalph E. Worthington, Michael A. Smith, John M. Tobias
Life of this patent
Estimating the term…
Abstract
Metals such as iron, uranium, vanadium, molybdenum and rare earths are reduced to lower oxidation states in various acid media using silicon metal or an iron-silicon alloy. In particular, ferric iron and hexavalent uranium in wet-process phosphoric acid are reduced to the ferrous and tetravalent states, respectively, using silicon metal or an iron-silicon alloy to provide a feed acid which is suitable for extraction with an extractant which is selective for tetravalent uranium such as a mixture of mono- and di-(alkylphenyl) esters of orthophosphoric acid.
Claims18
A process for reducing iron from the ferric to the ferrous state in wet-process phosphoric acid comprising contacting wet-process phosphoric acid containing ferric iron with a reductant selected from the group consisting of silicon metal and iron-silicon alloy containing about 5 to 80% silicon by weight to reduce at least a portion of said ferric iron in said wet-process phosphoric acid to the ferrous state.
A process for reducing iron from the ferric to the ferrous state in wet-process phosphoric acid comprising agitating wet-process phosphoric acid containing about 25 to 35% P.sub.2 O.sub.5 and ferric iron with a powdered reductant selected from the group consisting of silicon metal and iron-silicon alloy containing about 5 to 20% silicon by weight at a temperature of about 50.degree. C. to 80.degree. C. until at least a portion of said ferric iron is reduced to the ferrous state in said wet-process phosphoric acid and then removing any excess, unreacted reductant from said wet-process phosphoric acid.
A process for the recovery of uranium from wet-process phosphoric acid derived from the sulfuric acid acidulation of uncalcined phosphate rock comprising contacting wet-process phosphoric acid containing ferric iron and uranium values with a reductant selected from the group consisting of silicon metal and iron-silicon alloy containing about 5 to 80% silicon by weight to reduce ferric iron to ferrous iron and any hexavalent uranium to tetravalent uranium and contacting the reduced wet-process phosphoric acid with an organic extractant selective for uranium in the tetravalent state.
A process for reducing a metal to a lower oxidation state in an acid comprising contacting an acid selected from the group consisting of phosphoric acid, sulfuric acid and hydrochloric acid containing the metal selected from the group consisting of iron, uranium, vanadium, molybdenum and a rare earth with a reductant selected from the group consisting of silicon metal and iron-silicon all containing about 5 to 80% silicon by weight in the presence of fluoride ion to reduce at least a portion of said metal in said acid to a lower oxidation state.
A process for reducing a metal to a lower oxidation state in an acid comprising agitating an acid selected from the group consisting of phosphoric acid, sulfuric acid and hydrochloric acid containing a metal selected from the group consisting of iron, uranium, vanadium, molybdenum and a rare earth with a powdered reductant selected from the group consisting of silicon metal and iron-silicon alloy containing about 5 to 20% silicon by weight in the presence of fluoride ion in an amount of at least 1 gram/liter at a temperature of about 50.degree. C. to 80.degree. C. until at least a portion of said metal is reduced to a lower oxidation state in said acid and then removing any excess, unreacted reductant from said acid.