Galvanic cell with solid electrolyte
AssigneeVarta Batterie Aktiengesellschaft
InventorsRainer Bittihn, Armin Wagner, Jean-Paul Randin, Jean-Daniel Rosselet
Life of this patent
Estimating the term…
Loading patent…
AssigneeVarta Batterie Aktiengesellschaft
InventorsRainer Bittihn, Armin Wagner, Jean-Paul Randin, Jean-Daniel Rosselet
Estimating the term…
A galvanic cell with solid electrolyte, which is dischargeable at room temperature and whose positive electrode consists of the metals Sb, Bi, or of the oxides or chalcogenides of these metals, or of mixtures of members of the respective groups, bases its current productive processes upon the formation of a reversible inter-metallic combination between the Sb or Bi and the alkali metal of the negative electrode. The reaction equations are: 3Li+Bi=Li.sub.3 Bi or (1) 12 Li+Bi.sub.2 O.sub.3 =2 Li.sub.3 Bi+3Li.sub.2 O (2) A cathode material according to equation (2) is particularly desirable because Bi.sub.2 O.sub.3 has a higher volumetric capacity than Bi, due to the greater electron transition from Bi.sup.3+ to Bi.sup.3-, thereby yielding higher energy density. In both cases the discharge potential is 0.8 V. As the solid electrolyte, Li.sub.3 N or Na.sub.3 Zr.sub.2 Si.sub.2 PO.sub.12 (Nasicon) can be used.
A galvanic cell with solid electrolyte, having a negative lithium or sodium electrode, a solid positive electrode and a solid electrolyte between the electrodes and dischargeable at room temperature, wherein
Dependencies are inferred from the claim text.