Insulating fiber mixture, adhesive, and process
AssigneeFulbright & Jaworski
InventorsHarold F. Boyer, John L. Webb
Life of this patent
Estimating the term…
Abstract
A fiber adhesive is provided which is a mixture of sodium silicate and an acrylic resin, as well as a method for preparing the adhesive and spraying a mixture of the adhesive and the fiber.
Claims4
A process for applying an insulating mixture onto an object and for thereby building-up the insulating mixture on the object to a desired thickness, the process including
- mixing together in a container a fiber adhesive mixture of about 40% sodium silicate and about 60% acrylic resin and agitating them together sufficiently to form a homogenous mixture,
- mixing water with the adhesive mixture in a container so that the ratio of water to adhesive mixture is about 3.5 to 1 by volume,
- mixing insulating fiber with the adhesive-water mixture so that the ratio of fiber to adhesive-water mixture is about 1 lb. fiber to about 1/4 gallon adhesive-water mixture,
- introducing the fiber-water-adhesive mixture into an application apparatus, and
- applying the fiber-water-adhesive mixture onto an object to a desired thickness.
An insulating mixture for spraying onto an object to insulate the object and for thereby building up the insulating mixture on the object to a desired thickness, the insulating mixture comprising
- about 50% water,
- about 17% adhesive, the adhesive comprising about 40% sodium silicate and about 60% acrylic resin agitated together sufficiently to form a homogeneous mixture, and
- about 33% cellulose fiber.
An insulating mixture for spraying onto an object to insulate the object and for thereby building up the insulating mixture on the object to a desired thickness,
- the insulating mixture comprising about 50% water by weight, about 33% insulating fiber by weight and about 17% fiber adhesive by weight,
- the fiber adhesive comprising a mixture of sodium silicate and an acrylic resin, and the adhesive formed by sufficiently agitating the sodium silicate and acrylic resin together to form a homogeneous mixture.
A process for preparing an insulating mixture including the steps of
- providing a container
- mixing together in the container water, an adhesive including sodium silicate and an acrylic resin, and fiber,
- wherein the insulating mixture comprises about 50% water, about 33% fiber, and about 17% adhesive by weight.
Dependencies are inferred from the claim text.