Lube oil additive
AssigneeShell Oil Company
InventorRudolf J. A. Eckert
Life of this patent
Estimating the term…
Abstract
A modified hydrogenated star-shaped polymer comprising a nucleus, e.g., divinylbenzene, with polymeric arms linked to it is prepared by grafting a hydrogenated star-shaped polymer with a nitrogen-containing polymerizable polar organic compound, e.g., 2-vinylpyridine or 4-vinylpyridine. Such polymers are useful as viscosity index improvers for lube oil compositions, and also possess dispersancy.
Claims12
A modified hydrogenated star-shaped polymer comprising a poly-vinyl-aromatic nucleus and polymeric arms linked to said nucleus wherein said arms are selected from the group consisting of:
- (i) hydrogenated homopolymers and hydrogenated copolymers of conjugated dienes;
- (ii) hydrogenated copolymers of conjugated dienes and monoalkenyl arenes;
- and
- (iii) mixtures thereof;
- and wherein at least about 80% of the aliphatic unsaturation of the star-shaped polymer has been reduced by hydrogenation while less than 20% of the aromatic unsaturation has been reduced;
- and which star-shaped polymer has been grafted with a nitrogen containing polymerizable organic polar compound selected from the group consisting of piperidine, morpholine, piperazine, pyridine, pyrrolidone, pyrrole, benzopyrrole, quinoline, indole which are all alkenyl substituted and 2-methyl vinylpyridine and N-vinyl imidazole in the presence of a free radical polymerization initiator and wherein the number average molecular weight of each of said polymeric arms is from 5,000 to 150,000.
A process for preparing a dispersant/VI improver comprising reacting a selectively hydrogenated star-shaped polymer with a nitrogen containing polymerizable organic polar compound in the presence of a free radical polymerization initiator at a temperature of about 70.degree. C. to about 180.degree. C. and at a pressure of from 1 bar to 50 bar in an inert atmosphere wherein said star-shaped polymer comprises a poly(poly-vinyl-aromatic coupling agent) nucleus, and at least four polymeric arms linked to said nucleus wherein said polymeric arms are selected from the group consisting of:
- (i) hydrogenated homopolymers and hydrogenated copolymers of conjugated dienes;
- (ii) hydrogenated copolymers of conjugated dienes and monoalkenyl arenes;
- and
- (iii) mixtures thereof;
- and wherein at least about 80% of the aliphatic unsaturation of the star-shaped polymer has been reduced by hydrogenation while less than 20% of the aromatic unsaturation has been reduced, wherein said nitrogen compound is selected from the group consisting of piperidine, morpholine, piperazine, pyridine, pyrrolidone, pyrrole, benzopyrrole, quinoline, indole which are all alkenyl substituted and 2-methyl vinylpyridine and N-vinyl imidazole and wherein the number average molecular weight of each of said polymeric arms is from 5,000 to 150,000.
Dependencies are inferred from the claim text.