Hydrometallurgical treatment of copper-bearing hematite residue
AssigneeNoranda Mines Limited
InventorsRobert W. Stanley, Serge Monette, Derek G. E. Kerfoot
Life of this patent
Estimating the term…
Abstract
A method is provided for recovering copper values from a copper-bearing hematite residue in a single stage. It comprises leaching the residue in an aqueous sulphuric acid solution in the presence of ammonium, sodium or potassium ions, at a temperature between about 80.degree. C. and the boiling point of the solution so that copper values are dissolved while iron is precipitated as jarosite. The method is particularly suitable for the treatment of residues resulting from an oxidizing pressure leach of copper concentrates.
Claims4
A hydrometallurgical method of recovering copper values from copper concentrates which comprises:
- (a) forming an aqueous leach solution containing chloride or bromide ions in a predetermined concentration;
- (b) dispersing copper concentrates in said leach solution to form a slurry;
- (c) carrying out the leaching operation of said slurry at an elevated temperature and under an overpressure of oxygen as well as with the concentration of the chloride or bromide ions such as to transform a major portion of the copper values present in the concentrates into a solid basic copper sulphate;
- (d) separating resulting leach residue containing such basic copper sulphate from the leach solution;
- (e) dissolving said residue containing basic copper sulphate in a mild sulphuric acid leach to form a high-copper, low-iron solution;
- (f) separating said high-copper, low-iron solution from remaining hematite residue and purifying it to remove chloride or bromide ions and minor element impurities and then subjecting said purified solution to electrowinning for recovery of copper;
- (g) leaching the remaining hematite residue in an aqueous sulphuric acid solution and in the presence of ammonium, sodium and/or potassium ions to simultaneously solubilize copper values still remaining in the hematite residue, while converting a major portion of the hematite to ammonium, sodium and/or potassium jarosite thereby producing a low iron, copper-bearing solution containing less than 5 gpl dissolved iron therein;
- and
- (h) separating the resulting low-iron, copper-bearing solution from the jarosite containing residue and recycling it to the mild sulphuric acid leach step (e).
Dependencies are inferred from the claim text.