# US 4,338,137 A · Asphalt composition for air-blowing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,338,137 A
- Document ID: US4338137A
- Status: Granted
- Kind: A
- Application number: 06/285,248
- Filed: 1981-07-20
- Granted: 1982-07-06
- Earliest claimed: 1981-07-20
- Assignees: Chevron Research Company
- Inventors: Judson E. Goodrich
- Web page: https://patentgrep.com/patent/US4338137A

## CPC

- C10C 3/04: by blowing or oxidising {, e.g. air, ozone}
- C08K 3/16: Halogen-containing compounds
- C10C: WORKING-UP PITCH, ASPHALT, BITUMEN, TAR; PYROLIGNEOUS ACID (compositions of bituminous materials C08L95/00; carbon filaments by decomposition of organic filaments D01F9/14)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A process for air-blowing asphalt in the presence of ferrous chloride and an asphalt composition comprising a major amount of asphalt and a minor but effective amount of ferrous chloride.

## Claims

### Claim 1

An asphalt composition comprising 0.01 weight percent to about 5 weight percent ferrous chloride and asphalt in an amount to equal 100 weight percent.

### Claim 2 (depends on 1)

The composition according to claim 1 wherein the ferrous chloride is present in an amount of from about 0.10 to about 1 weight percent.

### Claim 3 (depends on 1)

The composition according to claim 1 wherein the ferrous chloride is hydrated.

### Claim 4

A process for producing blown asphalt which comprises air-blowing an asphalt in the presence of from about 0.01 weight percent to about 5 weight percent ferrous chloride for sufficient time to obtain a preselected softening point.

### Claim 5 (depends on 4)

A process according to claim 4 wherein the temperature is maintained within a range of from about 400.degree. to about 550.degree. F.

### Claim 6 (depends on 5)

A process according to claim 5 wherein the ferrous chloride is present in an amount of from about 0.1 weight percent to about 1 weight percent.

### Claim 7 (depends on 6)

The process according to claim 6 wherein the air-blowing is carried out for a period of about 0.5-12 hours.

### Claim 8 (depends on 7)

The process according to claim 7 wherein the ferrous chloride is added to the asphalt prior to air-blowing.

### Claim 9 (depends on 8)

The process according to claim 8 wherein the ferrous chloride is hydrated.

### Claim 10 (depends on 9)

The process according to claim 9 wherein the ferrous chloride is added to the asphalt at a temperature of from about 200.degree. to about 350.degree. F.