Defluorination of wet process phosphoric acid
AssigneeInternational Minerals & Chemical Corp.
InventorDennis H. Michalski
Life of this patent
Estimating the term…
Abstract
An improved method of defluorinating wet process phosphoric acid using silica-containing dust which is obtained as a waste product collected from the fumes of a submerged arc furnace process of making silicon metal alloys. The silica-containing dust has a very small particle size, and contains at least about 60% by weight silica (SiO.sub.2), and has a very high surface/mass ratio which increases the efficiency of the defluorination reaction. The defluorination reaction using this silica-containing fume takes less time than required using prior methods employing diatomaceous earth as the silica source. The presence of silicon metal alloy particles in the dust are thought to have a catalytic effect on the defluorination reaction.
Claims6
In a method of defluorinating phosphoric acid, in which concentrated wet process phosphoric acid is heated to boiling in the presence of silica to form water vapor and silicon tetrafluoride, the improvement comprising the step of contacting the phosphoric acid with an aqueous suspension comprising at least about 11% solids of a silica-containing dust collected as fume from silicon and silicon metal alloy furnace operations, said dust having a dry bulk density of less than about 10 lbs/ft.sup.3, and a silica content of at least about 60% by weight.
Dependencies are inferred from the claim text.