# US 4,325,770 A · Process for pressure-sensitive adhesive coated products

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,325,770 A
- Document ID: US4325770A
- Status: Granted
- Kind: A
- Application number: 06/163,606
- Filed: 1980-06-27
- Granted: 1982-04-20
- Earliest claimed: 1980-06-27
- Assignees: Permacel
- Inventors: Ralf Korpman
- Web page: https://patentgrep.com/patent/US4325770A

## CPC

- C09J 153/02: Vinyl aromatic monomers and conjugated dienes
- C09J 7/387: {Block-copolymers}
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

A process for making a pressure-sensitive adhesive coated product from an elastomer utilizing dry blending of powders and dry coating steps is described. Compositions suitable for use in this process are also described.

## Claims

### Claim 1

A process for making a pressure-sensitive adhesive coated product comprising:
(a) cooling a thermoplastic elastomer to below minus 20.degree. C. and pulverizing the cool polymer to a size sufficiently fine to pass through a 60 mesh screen to obtain an elastomer powder, said elastomer being an A-B-A block copolymer having a softening temperature maximum of no greater than about 233.degree. C.,
(b) pulverizing a tackifying resin of softening point in the range of about 85.degree. C. to about 150.degree. C. to a size sufficiently fine to pass through a 60 mesh screen to obtain a tackifier powder,
(c) dry blending at ambient temperature or below, said tackifier powder and elastomer powder in a weight ratio of about 50 to about 125 parts of tackifier powder to 100 parts of elastomer powder to obtain a blend of powders,
(d) dry coating said powder blend onto the surface of a substrate,
(e) heating the powder coated substrate to a temperature of at least about 177.degree. C. until the powder particles melt into union with each other to form a homogeneous molten coating, and
(f) allowing to cool to ambient temperature.

### Claim 2 (depends on 1)

A process according to claim 1 in which the thermoplastic elastomer is a (polystyrene-polyisoprene-polystyrene) or S-I-S block copolymer.

### Claim 3 (depends on 1)

A process according to claim 1 in which the thermoplastic elastomer is cooled and pulverized in liquid nitrogen.

### Claim 4 (depends on 1)

A process according to claim 1 in which the tackifier resin is selected from the group consisting of rosin, rosin derivatives, polymerized .alpha.- or .beta.-pinene, polyterpene, and polymerized mixture of piperylene and isoprene.

### Claim 5

A process for making a pressure-sensitive adhesive tape comprising:
(a) cooling a thermoplastic elastomer to below minus 20.degree. C. and pulverizing the cool polymer to a size sufficiently fine to pass through a 60 mesh screen to obtain an elastomer powder, said elastomer being an A-B-A block copolymer having a softening temperature maximum of no greater than about 233.degree. C.,
(b) pulverizing a tackifying resin of softening point in the range of about 85.degree. C. to about 150.degree. C. to a size sufficiently fine to pass through a 60 mesh screen to obtain a tackifier powder,
(c) dry blending at ambient temperature or below, said tackifier powder and elastomer powder in a weight ratio of about 50 to about 125 parts of tackifier powder to 100 parts of elastomer powder to obtain a blend of powders,
(d) dry coating said powder blend onto the surface of a sheet of heat-insensitive tape backing as substrate,
(e) heating the powder coated substrate to a temperature of at least about 177.degree. C. until the powder particles melt into union with each other to form a homogeneous molten coating, and
(f) allowing to cool to ambient temperature.

### Claim 6

A process for making pressure-sensitive adhesive tape comprising:
(a) cooling a thermoplastic elastomer to below minus 20.degree. C. and pulverizing the cool polymer to a size sufficiently fine to pass through a 60 mesh screen to obtain an elastomer powder, said elastomer being an A-B-A block copolymer having a softening temperature maximum of no greater than about 233.degree. C.,
(b) pulverizing a tackifying resin of softening point in the range of about 85.degree. C. to about 150.degree. C. to a size sufficiently fine to pass through a 60 mesh screen to obtain a tackifier powder,
(c) dry blending at ambient temperature or below, said tackifier powder and elastomer powder in a weight ratio of about 50 to about 125 parts of tackifier powder to 100 parts of elastomer powder to obtain a blend of powders,
(d) dry coating said powder blend onto the surface of a temporary substrate of carrier paper,
(e) heating the powder coated substrate to a temperature of at least about 177.degree. C. until the powder particles melt into union with each other to form a homogeneous molten coating,
(f) allowing to cool to ambient temperature to obtain an adhesive film, and
(g) transferring the adhesive to a heat-sensitive or porous tape backing.