Carrier-supported catalyst and process for making it
AssigneeHoechst Aktiengesellschaft
InventorsHeinz Erpenbach, Klaus Gehrmann, Herbert Joest
Life of this patent
Estimating the term…
Loading patent…
AssigneeHoechst Aktiengesellschaft
InventorsHeinz Erpenbach, Klaus Gehrmann, Herbert Joest
Estimating the term…
The invention relates to a carrier-supported catalyst comprising oxides of chromium and tungsten and at least one of the oxides of molybdenum and potassium in the atomic ratio of Cr.sub.1 W.sub.0.1-0.5 Mo.sub.0-0.05 K.sub.0-0.5 on a porous carrier material, and to a process for making it. To this end, the process provides (a) for a dry porous carrier material to be saturated with water up to 40 to 80% of its predetermined saturation value; (b) for the carrier material treated as under (a) to be impregnated in any sequential order, but at least once with an aqueous solution of water-soluble compounds of chromium and, if desired, potassium, and sequentially, but at least once with a separately produced aqueous solution of a water-soluble compound of tungsten and, if desired, molybdenum, the aqueous solutions being used in either case in a quantity which is at most necessary for complete saturation; (c) for the carrier material to be dried after each impregnation over a period of 2 to 20 hours at 350 to 500 K, and (d) for the carrier material to be sintered over a period of 0.5 to 12 hours at 550 to 1000 K, in a stream of air. The carrier-supported catalyst finds use in the production of styrene by subjecting ethylbenzene to oxidative dehydrogenation with molecular oxygen in gas phase.
A process for making a carrier-supported catalyst containing 2 to 30 weight % of the oxides of chromium and tungsten and of at least one of the oxides of molybdenum and potassium in the atomic ratio of Cr.sub.1 W.sub.0.1-0.5 Mo.sub.0-0.05 K.sub.0-0.5 on a porous carrier material selected from silicic acid or aluminum oxide, the carrier material having a BET-surface area of 2 to 200 m.sup.2 /g and consisting of particles with a size of 0.01 to 6 mm, which comprises:
A process for making a carrier-supported catalyst containing 2 to 30 weight % of the oxides of chromium and tungsten and of at least one of the oxides of molybdenum and potassium in the atomic ratio of Cr.sub.1 W.sub.0.1-0.5 Mo.sub.0-0.05 K.sub.0-0.5 on a porous carrier material selected from silicic acid or aluminum oxide, the carrier material having a BET-surface area of 2 to 200 m.sup.2 /g and consisting of particles with a size of 0.01 to 6 mm, which comprises: