Air-drying, fatty acid-modified lacquer binders, based on fumaric or maleic acid bis-glycidyl ester copolymers
AssigneeBayer Aktiengesellschaft
InventorsPeter Hohlein, Hans-Joachim Traenckner, Lothar Fleiter, Ludwig Bottenbruch
Life of this patent
Estimating the term…
Abstract
A binder composition which has a number average molecular weight of from 1000 to 20,000 and which comprises, in copolymerized form, from 5 to 55% by weight of fumaric acid and/or maleic acid bis-glycidyl ester and from 95 to 45% by weight of one or more vinyl and/or vinylidene monomers, esterified to an acid number of from 3 to 30 mg KOH/g with from 18 to 72% by weight, based on copolymer plus fatty acid, of a fatty acid and subsequently reacted with 0 to 3% by weight, based on copolymer plus fatty acid plus dicarboxylic acid anhydride, of a dicarboxylic acid anhydride.
Claims2
A binder composition having a number average molecular weight of from 1,000 to 20,000, said binder comprising a copolymer of from 5 to 55% by weight of at least one member selected from the group consisting of fumaric acid bis-glycidyl ester and maleic acid bis-glycidyl ester and from 95 to 45% by weight of at least one monomer selected from the group consisting of styrene, (meth)acrylic acid alkyl esters having from 1 to 8 carbon atoms in said alkyl moiety and mixtures thereof, said copolymer having been esterified to an acid number of from 3 to 30 mg KOH/g with from 18 to 72% by weight of a fatty acid, said percentage by weight being based on the total weight of said copolymer and said fatty acid and said esterified copolymer having been reacted with up to 3% by weight of dicarboxylic acid anhydride, said percentage by weight being based on the total weight of said copolymer, said fatty acid and said dicarboxylic acid anhydride.
A lacquer composition which comprises the binder of claim 2 and a lacquer solvent.
Dependencies are inferred from the claim text.