Process for spray cleaning of metal surfaces
AssigneeHenkel Kommanditgesellschaft auf Aktien
InventorsHerbert Lingmann, Hermann Drosdziok, Rudolf Peifer
Life of this patent
Estimating the term…
Abstract
A method of cleaning metal surfaces comprising spraying a metal surface with an aqueous solution containing (a) at least one soluble salt of a carboxylic acid having 6 to 12 carbon atoms selected from the group consisting of aromatic carboxylic acids, aliphatic carboxylic acids and mixtures thereof, (b) at least one nonionic surface-active compound, (c) at least one quaternary ammonium surface-active compound, where the concentration of the active-substances (a), (b) and (c) in the aqueous solution is from 0.1% to 4% by weight and the weight ratio of (b) to (c) is from 20:1 to 1:1 and the weight ratio of (a) to (b)+(c) is from 20:1 to 1:20, where the pH of the aqueous solution is from 7.5 to 11.
Claims8
A method of cleaning metal surfaces comprising spraying a metal surface at a pressure of 10 atmospheres gauge or higher with an aqueous solution consisting essentially of water containing a mixture of active substances of
- (a) at least one water-soluble alkanolamine salt of alkanolamines having 2 to 9 carbon atoms, of monocarboxylic acids selected from the group consisting of benzoic acid, tertiary butylbenzoic acid, phenylacetic acid, cinnamic acid, caprylic acid, capric acid, isooctanoic acid, isononanoic acid, isodecanoic acid and mixtures thereof,
- (b) at least one nonionic surface-active compound having an HLB value of between 14 and 20, and
- (c) at least one quaternary ammonium surface-active compound, wherein the concentration of the mixture of active substances (a), (b) and (c) in the aqueous solution is from 0.1% to 4% by weight, the weight ratio of (b) to (c) is from 20:1 to 1:1, the weight ratio of (a) to (b)+(c) is from 20:1 to 1:20, and sufficient alkanolamine having 2 to 9 carbon atoms is present whereby the pH of the aqueous solution is from 7.5 to 11, wherein the aqueous solution is maintained at a preselected temperature between 20.degree. C. and 80.degree. C. and the components (a), (b) and (c) are so selected that the turbidity point of said aqueous solution lies from 5.degree. C. to 25.degree. C. below said preselected temperature.
In the industrial process for cleaning of metal parts in a spray-washing plant comprising spraying said metal parts at a pressure of 10 atmospheres gauge or higher with a recirculated washing fluid in a spraying zone, rinsing said metal parts in a rinsing step and recovering said cleaned metal parts, the improvement comprising employing an aqueous solution consisting essentially of water, containing a mixture of active substances of:
- (a) at least one water-soluble alkanolamine salt of alkanolamines having 2 to 9 carbon atoms, of monocarboxylic acids selected from the group consisting of benzoic acid, tertiary butylbenzoic acid, phenylacetic acid, cinnamic acid, caprylic acid, capric acid, isooctanoic acid, isononanoic acid, isodecanoic acid and mixtures thereof,
- (b) at least one nonionic surface-active compound having an HLB value of between 14 and 20, and
- (c) at least one quaternary ammonium surface-active compound, wherein the concentration of the mixture of active substances (a), (b) and (c) in the aqueous solution is from 0.1% to 4% by weight, the weight ratio of (b) to (c) is from 20:1 to 1:1, the weight ratio of (a) to (b)+(c) is from 20:1 to 1:20, and sufficient alkanolamine having 2 to 9 carbon atoms is present whereby the pH of the aqueous solution is from 7.5 to 11, wherein the aqueous solution is maintained at a preselected temperature between 20.degree. C. and 80.degree. C. and the components (a), (b) and (c) are so selected that the turbidity point of said aqueous solution lies from 5.degree. C. to 25.degree. C. below said preselected temperature, as said recirculated washing fluid, whereby no foaming or precipitation of tensides occurred over spray periods of at least five days.
Dependencies are inferred from the claim text.