# US 4,248,652 A · Method of making leatherlike materials (A)

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,248,652 A
- Document ID: US4248652A
- Status: Granted
- Kind: A
- Application number: 06/041,779
- Filed: 1979-05-23
- Granted: 1981-02-03
- Earliest claimed: 1978-03-30
- Assignees: Inmont Corporation
- Inventors: Frank P. Civardi; Stanley G. Sova; Bohdan V. Burachinsky
- Web page: https://patentgrep.com/patent/US4248652A

## CPC

- B32B 27/12: next to a fibrous or filamentary layer
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 27/40: comprising polyurethanes
- D06N 3/0077: {Embossing; Pressing of the surface; Tumbling and crumbling; Cracking; Cooling; Heating, e.g. mirror finish}
- D06N 3/14: with polyurethanes
- B32B 2305/026: Porous
- Y10S 428/904: Artificial leather
- Y10T 156/1039: Surface deformation only of sandwich or lamina [e.g., embossed panels]
- Y10T 156/1041: Subsequent to lamination
- Y10T 428/24438: Artificial wood or leather grain surface
- Y10T 428/24998: Composite has more than two layers
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- D06N: WALL, FLOOR, OR LIKE COVERING MATERIALS, e.g. LINOLEUM, OILCLOTH, ARTIFICIAL LEATHER, ROOFING FELT, CONSISTING OF A FIBROUS WEB COATED WITH A LAYER OF MACROMOLECULAR MATERIAL; FLEXIBLE SHEET MATERIAL NOT OTHERWISE PROVIDED FOR
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A system for the manufacture of leatherlike materials, particularly for shoe uppers, which avoids pollution, toxicity and fire hazards and makes it possible for the shoe manufacturer to make his shoe upper materials as required with a minimum of investment in inventory of raw materials and with simple, relatively inexpensive equipment.

## Claims

### Claim 1

Process for making artificial leather which comprises
(a) providing a supply of continuous web of fibrous material and a separate supply of continuous sheet of microporous elastomeric polyurethane
(b) continuously pulling said web and sheet lengthwise under tension from said supplies and assembling said web and sheet together in face-to-face relationship under tension
(c) maintaining an adhesive material in heat-softened condition at the interface between said web and said sheet and in adhesive contact with said sheet,
(d) placing a thin preformed skin on the outer surface of said microporous polyurethane, said skin having a surface, in contact with said microporous outer surface, which is heat fusible to said outer surface,
(e) passing the resulting assemblage continuously lengthwise onto a rotating embossing roll having a hot grain-embossing surface in contact with said skin at a temperature above the temperature at which said skin fuses to said outer surface, and
(f) continuously removing said assemblage lengthwise from said embossing roll.

### Claim 2 (depends on 1)

Process as in claim 1 and including the further step of
(g) maintaining said assemblage under substantial absence of tension and in lengthwise arcuate form with its grained surface convex at an elevated temperature such as to cause lengthwise relaxation of the microporous material thereby causing said fibrous web laminated thereto to undergo lengthwise contraction.

### Claim 3 (depends on 1)

Process as in claim 1 in which said heat softened adhesive material is adhered in a discontinuous or open pattern to said sheet.

### Claim 4 (depends on 1)

Process as in claim 1 in which said skin is heat-adhered to said outer surface of said microporous polyurethane prior to said step e.

### Claim 5 (depends on 1)

Process as in claim 1 including the steps of providing a supply of a continuous supporting film carrying said skin, continuously drawing off said skin-carrying film from said supply onto the surface of a rotating roll having a hot surface in contact with said supporting film at a temperature above said skin-outer surface fusion temperature and maintaining said outer surface of said microporous polyurethane in contact with said skin on said film-contacted roll so as to adhere said skin to said outer microporous surface, and thereafter stripping said film from said assemblage prior to said step e.

### Claim 6 (depends on 5)

Process as in claim 5 in which said film is of polyethylene terephthalate.

### Claim 7 (depends on 1)

Process as in claim 1 in which said fusible surface of said skin is of elastomeric polyurethane having a lower melting point than the polyurethane of said outer microporous surface.

### Claim 8 (depends on 1)

Process as in claim 1 in which the face of said skin which is in contact with said embossing surface carries a release agent.

### Claim 9 (depends on 1)

Process as in claim 1 in which in said step e said assemblage passes through the nip between said embossing roll and an elastomer surfaced roll biased toward said embossing roll, the conditions being such that at said nip said microporous polyurethane is compressed and said elastomer roll surface is deformed, said microporous polyurethane then expands to substantially its original thickness on leaving said nip and said assemblage, with said skin, then remains in contact with said embossing roll for a period of at least about 1/2 second, the residence time in said nip being less than about 0.1 second.

### Claim 10 (depends on 9)

Process as in claim 9 in which said hot grain-embossing surface is at a temperature within about 15.degree. C. of the melting-sticking temperature of said microporous material.

### Claim 11 (depends on 1)

Process as in claim 1 in which the weight ratio of fibrous material to elastomer in said assemblage is about 0.8:1 to 1.2:1 and the thickness of said assemblage is about 20 to 80 mils.

### Claim 12 (depends on 5)

Process as in claim 5 in which said skin comprises a plurality of layers including a layer adjacent to said film and carrying a release agent to reduce adhesion to said embossing surface and another layer, further from said film than said first mentioned layer, of elastomeric polyurethane.

### Claim 13

Process for making artificial leather which comprises
(a) providing a supply of continuous web of fibrous material and a separate supply of continuous sheet of microporous elastomeric polyurethane
(b) continuously pulling said web and sheet lengthwise under tension from said supplies and assembling said web and sheet together in face-to-face relationship under tension
(c) maintaining an adhesive material in heat-softened condition at the interface between said web and said sheet and in adhesive contact with said sheet
(d) passing the resulting assemblage continuously lengthwise onto a rotating embossing roll having a hot grain-embossing surface in contact with the outer surface of said microporous polyurethane at a temperature within about 15.degree. C. of the melting-sticking temperature of said outer surface, and
(e) continuously removing said assemblage lengthwise from said embossing roll.

### Claim 14 (depends on 13)

Process as in claim 13 and including the further step of
(f) maintaining said assemblage under substantial absence of tension and in lengthwise arcuate form with its grained surface convex at an elevated temperature such as to cause lengthwise relaxation of the microporous material thereby causing said fibrous web laminated thereto to undergo lengthwise contraction.

### Claim 15 (depends on 13)

Process as in claim 13 in which in said step d said assemblage passes through the nip between said embossing roll and an elastomer surfaced roll biased toward said embossing roll, the conditions being such that at said nip said microporous polyurethane is compressed and said elastomer roll surface is deformed, said microporous polyurethane then expands to substantially its original thickness on leaving said nip and said assemblage, with said skin, then remains in contact with said embossing roll for a period of at least about 1/2 second, the residence time in said nip being less than about 0.1 second.

### Claim 16 (depends on 15)

Process as in claim 15 in which said hot grain-embossing surface is at a temperature within about 15.degree. C. of the melting-sticking temperature of said microporous polyurethane.

### Claim 17 (depends on 11)

Process as in claim 11 in which said microporous sheet is about 10 to 50 mils thick and has a specific gravity of about 0.3 to 0.5 and is produced by coagulating a layer of a solution of said elastomeric polyurethane in a liquid solvent by contacting said layer with a non-solvent miscible with said solvent.

### Claim 18 (depends on 10)

Process as in claim 10 in which said microporous sheet is about 10 to 50 mils thick and has a specific gravity of about 0.3 to 0.5 and in which the weight ratio of fibrous material to elastomer in said assemblage is about 0.8:1 to 1.2:1 and the thickness of said assemblage is about 20 to 80 mils.

### Claim 19 (depends on 14)

Process as in claim 14 in which said microporous sheet is about 10 to 50 mils thick and has a specific gravity of about 0.3 to 0.5 and in which the weight ratio of fibrous material to elastomer in said assemblage is about 0.8:1 to 1.2:1 and the thickness of said assemblage is about 20 to 80 mils.

### Claim 20 (depends on 15)

Process as in claim 15 in which said microporous sheet is about 10 to 50 mils thick and has a specific gravity of about 0.3 to 0.5 and in which the weight ratio of fibrous material to elastomer in said assemblage is about 0.8:1 to 1.2:1 and the thickness of said assemblage is about 20 to 80 mils.