Ink composition for non woven fabrics of synthetic fibers
AssigneeATEX/U.S.A., Inc.
InventorMaurizio Giorgetti
Life of this patent
Estimating the term…
Abstract
An ink composition is provided for the lithographic imprinting of non woven fabrics constituted of polyethylene fibers, such a composition comprising a pigment, a desiccant, a binder based on isophthalic and/or urethane varnish, a protective wax and an oleoresinous varnish consisting of phenolic resin, linseed oil, tung oil and high boiling mineral oil.
Claims6
An ink composition for the imprinting of polyolefinic non woven fabrics, comprising a pigment, a desiccant, a binder based on isophthalic and/or urethane varnish, a polyethylene protective wax and characterized in that it comprises between 54 and 64 percent by weight of an oleoresinous varnish consisting of a phenolic resin, crude linseed oil, tung oil and high boiling mineral oil, the composition being further characterized in that it imparts significant resistance to washing of the polyolefinic non woven fabrics such that when said fabric is washed as a delicate textile with a bland detergent, no discernible color change occurs after as many as six or seven cycles of washing, the composition being further characterized in that it imparts a feel or "hand" to said imprinted polyolefinic non woven fabric which remains unchanged after repeated washings and prolonged period of storage, the composition being further characterized in that said imprinted polyolefinic non woven fabric demonstrates substantial resistance to abrasion, the composition being further characterized in that said imprinting of polyolefinic non woven fabrics can be carried out lithographically with a desiccation time substantially less than two days, and characterized by a durable chemical linkage between the ink and the non woven fabric such that breakage does not occur under flexing of the fabric.
An ink composition for the imprinting of polyolefinic non woven fabrics comprising (percentages by weight)
- ______________________________________ a pigment 10-20% isophthalic varnish 10% urethane varnish 8% oleoresinous varnish 54-64% polyethylene wax 3% cobalt manganese-naphthenate desiccant 3% ______________________________________
A process for making an ink composition for the imprinting of polyolefinic non woven fabrics, comprising the following steps:
- (a) preparing an oleoresinous varnish by heating at 220.degree. C. in an open cauldron 39 parts of phenolic resin, 20 parts of neutral bleached linseed oil, 10 parts of tung oil prepared at 230.degree. C., and 31 parts of high boiling mineral oil prepared at 190.degree. C.;
- (b) mixing the components from step (a) for about 50 minutes;
- (c) unloading and subjecting the mixture from step (b) to refining in a conventional refining device having three cylinders with a minimum of three passages;
- (d) adding to the product of (c) 23 parts of the same oleoresinous varnish of step (a), together with 3 parts of a desiccant comprising cobalt, manganese-naphthenate;
- (e) removing the product of step (d) for utilizing in lithographic imprinting of said non woven polyolefinic fabric.
Dependencies are inferred from the claim text.