Process for urea granulation
AssigneeCompagnie Neerlandaise de l'Azote
InventorsAnton Niks, Willy H. P. Van Hijfte, Rafael A. J. Goethals
Life of this patent
Estimating the term…
Abstract
Urea granules are prepared by spraying an aqueous urea solution having a urea concentration of 70-99.9% by weight on to fluidized urea nuclei in the form of droplets having a mean drop diameter of 20-120 .mu.m at a temperature at which the water is evaporated from the solution sprayed on to the nuclei and urea crystallizes on the nuclei to form granules having a desired size.
Claims11
A process for producing urea granules, characterized by spraying an aqueous solution consisting essentially of urea having a urea concentration of 70-99.9% by weight onto fluidized urea nuclei in the form of droplets having a mean drop diameter of 20-120 .mu.m at a temperature at which the water is evaporated from the solution sprayed onto the nuclei, and urea crystallizes on the nuclei, to form granules having a desired size.