# US 4,159,358 A · Method of bonding a bioglass to metal

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,159,358 A
- Document ID: US4159358A
- Status: Granted
- Kind: A
- Application number: 05/798,671
- Filed: 1977-05-19
- Granted: 1979-06-26
- Earliest claimed: 1977-05-19
- Assignees: Board of Regents, State of Florida
- Inventors: Larry L. Hench; Paul J. Buscemi
- Web page: https://patentgrep.com/patent/US4159358A

## CPC

- C03C 4/0007: {for biologically-compatible glass}
- A61C 8/0012: {characterised by the material or composition, e.g. ceramics, surface layer, metal alloy (use of specific materials A61K6/00)}
- A61C 8/0013: {with a surface layer, coating}
- A61F 2/30767: {Special external or bone-contacting surface, e.g. coating for improving bone ingrowth}
- A61L 27/306: {Other specific inorganic materials not covered by A61L27/303 - A61L27/32}
- A61L 27/32: Phosphorus-containing materials, e.g. apatite
- C03C 27/02: by fusing glass directly to metal
- C23D 5/04: by dry methods
- A61F 2310/00796: Coating or prosthesis-covering structure made of a phosphorus-containing compound, e.g. hydroxy(l)apatite
- A61F 2310/00928: Coating or prosthesis-covering structure made of glass or of glass-containing compounds, e.g. of bioglass
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- A61C: DENTISTRY; APPARATUS OR METHODS FOR ORAL OR DENTAL HYGIENE (non-driven toothbrushes A46B; {tongue scrapers A61B17/24;} preparations for dentistry A61K6/00; preparations for cleaning the teeth or mouth A61K8/00, A61Q11/00)
- A61F: FILTERS IMPLANTABLE INTO BLOOD VESSELS; PROSTHESES; DEVICES PROVIDING PATENCY TO, OR PREVENTING COLLAPSING OF, TUBULAR STRUCTURES OF THE BODY, e.g. STENTS; ORTHOPAEDIC, NURSING OR CONTRACEPTIVE DEVICES; FOMENTATION; TREATMENT OR PROTECTION OF EYES OR EARS; BANDAGES, DRESSINGS OR ABSORBENT PADS; FIRST-AID KITS (dental prosthetics A61C)
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- C23D: ENAMELLING OF, OR APPLYING A VITREOUS LAYER TO, METALS

## Abstract

A method of bonding a bioglass layer to a metal substrate comprising heating the metal substrate having a roughened, oxidized surface to about a temperature at which the expansion of the metal is substantially equal to that of the bioglass at the temperature above which the thermal expansion of the bioglass is non-linear, immersing the heated metal surface in molten bioglass, the time of immersion being of such duration that the temperature of the metal does not rise substantially above the temperature to which it is heated, allowing the coated substrate to cool whereby the bioglass layer is bonded to the metal substrate by ion diffusion and thermo-mechanical stresses in the bioglass and metal layer are relieved at a substantially equal rate and the product produced by said process.

## Claims

### Claim 1

A method of bonding a bioglass layer to a metal substrate comprising:
(1) heating a metal substrate having a roughened, oxidized surface to about a maximum temperature (T.sub.1) where said T.sub.1 is selected such that the total volume expansion of said metal is substantially equal to that of said bioglass at the temperature (T.sub.s) at which the temperature dependence of the volume of said bioglass becomes non-linear,
(2) providing a body of molten bioglass at temperature T.sub.w where T.sub.w is sufficiently high that the said bioglass is sufficiently fluid to allow immersion of said metal heated to temperature T.sub.1,
(3) immersing said metal surface in said molten bioglass for the minimum time required to permit a layer of desired thickness of said bioglass to adhere to said surface upon termination of said immersion, the time of said immersion being of such duration that the temperature of said metal surface does not rise substantially above T.sub.1,
(4) terminating said immersion,
(5) allowing said coating to cool rapidly from T.sub.w to about T.sub.s, whereby the thermo-mechanical stresses in said bioglass layer are rapidly relieved, and
(6) allowing said coated substrate to further cool to a temperature below about T.sub.s, whereby the thermo-mechanical stresses in said bioglass coating and said metal surface are relieved at a substantially equal rate due to the substantially linear thermal expansions thereof,
said bioglass coating being bonded to said metal surface by ion diffusion through said oxidized surface.

### Claim 2 (depends on 1)

The method of claim 1 wherein a predetermined viscosity of the molten bioglass, prior to immersion, is maintained by temperature adjustment in order to control the desired thickness of said adhered layer of bioglass on said metal surface.

### Claim 3 (depends on 2)

The method of claim 2 wherein the temperature of said molten bioglass is maintained at between about 1250.degree. C. to about 1550.degree. C.

### Claim 4 (depends on 1)

The method of claim 1 wherein said T.sub.1 is above about 700.degree. C.

### Claim 5 (depends on 1)

The method of claim 1 wherein said metal surface has a degree of roughness below that at which mechanical interlocking between said metal surface and said bioglass coating occurs.

### Claim 6 (depends on 1)

The method of claim 1 including the step of oxidizing said roughened metal surface.

### Claim 7 (depends on 6)

The method of claim 6 wherein said metal surface is oxidized by exposing said metal surface to an oxidizing temperature at an elevated temperature.

### Claim 8 (depends on 1)

The method of claim 1, wherein said metal is a steel, a cobalt-chrome alloy, titanium or titanium alloy, a noble metal or noble metal alloy, or a molybdenum-nickel-cobalt-chrome alloy.

### Claim 9 (depends on 8)

The method of claim 8 wherein said steel is stainless steel.

### Claim 10 (depends on 8)

The method of claim 8 wherein said steel is carbon steel.

### Claim 11 (depends on 1)

The method of claim 1 wherein said bioglass has a moderately high alkali content and is substantially invert with respect to silica content.

### Claim 12 (depends on 11)

The method of claim 11 wherein said bioglass contains, by weight:
SiO.sub.2 --40-62%
Na.sub.2 O--10-32%
Ca0--10-32%
P.sub.2 o.sub.5 --0-12%
caF.sub.2 --0-18%
B.sub.2 o.sub.3 --0-20%.

### Claim 13 (depends on 1)

the method of claim 1 wherein said biologically active glass contains, by weight:
SiO.sub.2 --45.0%
Na.sub.2 O--24.5%
CaO--24.5%
P.sub.2 o.sub.5 --6.0%.

### Claim 14 (depends on 1)

the method of claim 1 wherein said biologically active glass contains, by weight:
SiO.sub.2 --42.94%
Na.sub.2 O--23.37%
CaO--11.69%
P.sub.2 o.sub.5 --5.72%
caF.sub.2 --16.26%.

### Claim 15 (depends on 1)

The method of claim 1 wherein said biologically active glass contains, by weight:
SiO.sub.2 --40.0%
Na.sub.2 O--24.5%
CaO--24.5%
P.sub.2 o.sub.5 --6.0%
b.sub.2 o.sub.3 --5.0%.

### Claim 16 (depends on 1)

the method of claim 1 wherein the thickness of said bioglass coating is from about 0.2mm to about 2mm.

### Claim 17 (depends on 1)

The method of claim 1 wherein the time of immersion is less than about 5 seconds.

### Claim 18 (depends on 6)

The method of claim 6 wherein said metal is a steel and is oxidized by exposure to air at about 800.degree. C. for about 20 minutes.
