Abstract
A self-swelling leakage-preventing material is produced by reacting under heat a mixture of a copolymer of a lower olefin such as isobutene with maleic anhydride, a polymer emulsion having compatibility with the copolymer, such as an ethylene-vinyl acetate copolymer emulsion, and a compound having at least two functional groups selected from the group consisting of hydroxyl groups, amino groups and epoxy groups, such as ethylene glycol, until a cross-linked product having a swelling rate of 5-40 times is obtained. The mixture itself may be shaped into a suitable form prior to the reaction. A core material such as a non-woven fabric may be impregnated with the mixture prior to the reaction.
Claims7
A process for the production of a self-swelling leakage-preventing material, characterized by reacting under heat a mixture of a copolymer of a lower olefin and maleic anhydride, an ethylene-vinyl acetate copolymer emulsion having a compatibility with said copolymer, and a compound having at least two functional groups selected from the group consisting of hydroxy groups, amino groups and epoxy groups, until a crosslinked product having a swelling rate of 5-40 times is obtained, about 20 to 100 parts of the ethylene-vinyl actetate copolymer being employed per 100 parts by weight of the olefin-maleic anhydride copolymer.
Dependencies are inferred from the claim text.