Priming mix with minimum viscosity change
AssigneeOlin Corporation
InventorEugene A. Andrew
Life of this patent
Estimating the term…
Abstract
An extrudable ammunition priming mix with viscosity characteristics which remain relatively stable over an extended time span. The stabilized viscosity is obtained by incorporating an effective amount of guar gum into the priming mix. The primer thus displays improved pot life so that larger batches may be made and used over an extended period of time.
Claims6
A water-bearing extrudable explosive primer mix having improved rheological stability comprising:
- (a) about from 25 to 60% lead styphnate,
- (b) about from 1 to 10% tetracene,
- (c) about from 0 to 10% pentaerythritol tetranitrate (PETN),
- (d) about from 20 to 60% barium nitrate,
- (e) about from 0 to 25% antimony sulfide,
- (f) about from 0 to 10% aluminum,
- (g) an amount of water effective to reduce said mix to an extrudable consistancy, and
- (h) an amount of guar gum effective to substantially stabilize the consistancy of said extrudable mix.
5 more elements
An extrudable ammunition primer mix having improved rheological stability comprising:
- effective amounts of at least one primary explosive, at least one oxidizer, and at least one fuel;
- an amount of water effective to provide said primer mix with a readily extrudable consistancy and viscosity;
- and an effective amount of guar gum to substantially stabilize the consistancy and viscosity of said primer mix.