The fluoride values of fluorapatite ores can be recovered by using reactive metal compounds, e.g., the sulfates, phosphates or hydroxides of aluminum, iron, titanium, zirconium, antimony or chromium, to tie up the fluorides during acid attack on the ores and thus minimize the formation of fluosilicic acid. The soluble metal fluoride salts formed can subsequently be separated and treated with acid to recover hydrogen fluoride.
Claims2
A method for treating fluorapatite ore to recover fluoride values contained therein, said method consisting essentially of
- (1) subjecting said ore to aqueous mineral acid attack to convert the phosphate contained in the ore to phosphoric acid in the presence of an added reactive metal compound selected from the group consisting of chloride, nitrate, sulfate, phosphate, bromide, perchlorate, hydroxyacetate, acetate, carbonate or hydroxide of aluminum, titanium, zirconium and trivalent iron, to convert the fluoride contained in the ore into a water-soluble fluoride complex in which a substantial portion remains in solution in the reaction medium and which is sufficiently stable to prevent the formation of fluosilicic acid, said amount of reactive metal compound being present in a molar ratio of reactive metal compound to fluorine content in said ore of from about 1/(V + 3):1 to 2:1, where V is the valence of the reactive metal cation;
- and
- (2) adding sufficient alcohol having from 1 to 4 carbon atoms to obtain a phase separation of the fluoride complex from the phosphoric acid-alcohol solution.
Dependencies are inferred from the claim text.