Composition for the decomposition of sodium-mercury amalgam
AssigneeOlin Corporation
InventorHarshad M. Patel
Life of this patent
Estimating the term…
Abstract
A method and composition are described for the decomposition of sodium-mercury amalgam in a reactor containing solid packing particles to form hydrogen, sodium hydroxide, and denuded mercury. The novel packing particles are comprised of a heterogeneous solid mixture of a matrix of a thermally stable polymer having embedded therein discrete particles of a surface active composition. Suitable thermally stable polymers include polyphenylene sulfide and suitable surface active compositions include carbon, iron, nickel, cobalt, vanadium, and molybdenum. The proportion of the polymer in the packing generally ranges from about 20 to about 80 percent by volume. Preferably, the matrix is prepared in porous form which may also be coated with a surface active metal.
Claims12
Granular packing for decomposing sodium-mercury amalgam comprised of a solid mixture of a thermally stable porous polymer matrix having embedded therein discrete particles of a surface active composition, wherein said surface active composition is selected from the group consisting of iron, cobalt, nickel, graphite, molybdenum, vanadium and mixtures thereof, wherein the proportion of said thermally stable polymer to said particles of surface active composition is in the range from about 20 to about 80% by volume of the resulting dispersion, wherein said thermally stable polymer is selected from the group consisting of polyphenylene sulfide, polyphenylene oxide, phenolic resins, polymers of furfuryl alcohols, imid polymers, silicone polymers, epoxy polymers, furan polymers, urethane polyphenylene sulfides, polyvinylidene fluorides, polyacrylonitrile, and polyvinyl alcohol, and wherein the particle size of said surface active composition is in the range from about 75 to about 1,000 microns.
Dependencies are inferred from the claim text.