Process for recovery of mineral values from underground formations
AssigneeUnion Oil Company of California
InventorWilliam E. Showalter
Life of this patent
Estimating the term…
Abstract
Carbon dioxide is admixed with water to form a carbonic acid solution for use as a leaching solution for extraction of uranium by solution mining. An oxidizing agent is also present in the solution.
Claims25
In a method for the solution mining of a substance which in an oxidized state is soluble in an aqueous leaching solution, said method comprising the steps of (1) introducing an oxidant and an aqueous leaching solution into a subterranean deposit containing said substance, thereby to solubilize said substance in situ to form a pregnant liquor, (2) recovering said pregnant liquor from said deposit, and (3) separating said substance from said pregnant liquor, the improvement comprising:
- utilizing as said aqueous leaching solution a solution comprising a dilute aqueous carbonic acid solution and said oxidant.
A method for the recovery of uranium values from a subterranean formation comprising the steps of:
- introducing a leaching solution comprising a dilute aqueous carbonic acid solution containing an oxidizing agent for said uranium values into said subterranean formation wherein said uranium values are solubilized in said leaching solution to form a pregnant liquor, the concentration of said carbonic acid in said leaching solution being sufficient to provide a bicarbonate ion concentration in said leaching solution between about 380 ppm and about 1000 ppm and said leaching solution having a pH of less than about 7;
- thereafter recovering said pregnant liquor from said formation;
- and
- separating and recovering said uranium values from said pregnant liquor.
A process for the recovery of uranium values from a subterranean deposit comprising the steps of:
- (a) penetrating said deposit with at least one injection well and at least one production well in spaced relation with said injection well;
- (b) introducing an aqueous leaching solution comprising carbonic acid and an oxidizing agent selected from the group consisting of hydrogen peroxide, oxygen and oxygen-containing gases from said injection well into said deposit to leach in situ uranium values therefrom thereby forming a pregnant liquor, the concentration of said carbonic acid in said leaching solution being sufficient to provide a bicarbonate ion concentration in said leaching solution between about 380 ppm and about 1000 ppm and the concentration of said oxidizing agent in said leaching solution being between about 50 ppm and about 200 ppm on a free oxygen basis;
- (c) recovering said pregnant liquor at said production well;
- (d) forming a barren liquor by separating said uranium values from said pregnant liquor;
- (e) introducing gaseous carbon dioxide and said oxidizing agent into said barren liquor thereby to form said aqueous leaching solution;
- and
- (f) recycling at least a portion of the solution formed in step (e) for reintroduction into said deposit in step (b).
In the solution mining of substances from a subterranean formation using an alkaline carbonate leaching solution wherein the leaching solution is introduced into an injection well for percolation through the formation and the solution containing dissolved substance is recovered from a production well spaced from said injection well, a method for increasing the injectivity of said injection well comprising injecting an aqueous solution of an oxidizing agent into the injection well and simultaneously introducing gaseous carbon dioxide into the injection well.
Dependencies are inferred from the claim text.