Process for coagulating polymer latices using screw-type extruder
AssigneeInternational Basic Economy Corporation
InventorsDouglas Leo Hertel, Robert Wen Lee
Life of this patent
Estimating the term…
Abstract
A polymer latex is coagulated by passing the polymer latex and a coagulant through a screw-type extruder in which the latex and coagulant are mixed and mechanically worked under pressure by a rotating interrupted worm flight in cooperation with a plurality of stationary breaker members. At the downstream end of the extruder, the coagulated polymer is compacted and extruded. The extruded polymer is characterized by relatively low moisture content, and the excess process liquid which drains from the compacted polymer is relatively free of uncoagulated polymer.
Claims16
The process of coagulating a polymer latex comprising mixing and mechanically working the polymer latex and a coagulant under pressure in an extruder to produce a coagulated polymer having moisture content less than 25% by weight, the extruder including an elongated chamber, an axial rotating interrupted worm flight disposed in the chamber for initially contacting and mixing the polymer latex and coagulant in the worm flight to form a coagulating mixture and for advancing the coagulating mixture through the chamber to an extruder exit, and a plurality of stationary breakers projecting into the interior of the chamber intermediate at least some of the segments of the interrupted worm flight, the interrupted worm flight and the breakers cooperating to maintain the coagulating mixture under pressure in the worm flight at least until coagulation of the polymer latex is substantially complete, the segments of the interrupted worm flight and the breakers also cooperating to turbulently mix and mechanically work the constituents of the pressurized coagulating mixture in the worm flight and to break up any coagulated polymer encapsulating uncoagulated polymer latex and release the encapsulated polymer latex for mixture with coagulant, and extruding the coagulated polymer from the extruder exit with a moisture content less than 25% by weight.
The process of coagulating a polymer latex comprising the steps of:
- introducing separate streams of the polymer latex and a coagulant into the spaces between the upstream segments of a rotating interrupted worm flight axially disposed in an elongated pressurized chamber to form a pressurized coagulating mixture in the spaces between the worm flight segments in the chamber;
- advancing the coagulating mixture from the upstream portion of the chamber through the spaces between the worm flight segments to the downstream portion of the chamber by rotation of the interrupted worm flight disposed in the chamber;
- maintaining the advancing coagulating mixture under pressure in the spaces between the worm flight segments at least until coagulation of the polymer latex is substantially complete by cooperation of the segments of the interrupted worm flight and a plurality of fixed breakers projecting into the spaces intermediate at least some of the segments of the interrupted worm flight;
- turbulently mechanically working the pressurized coagulating mixture in the spaces between the worm flight segments to thoroughly and intimately mix the constituents of the mixture and to release any uncoagulated polymer latex which has been encapsulated by coagulated polymer by cooperation of the segments of the interrupted worm flight and the fixed breakers to produce a coagulated polymer having moisture content less than 25% by weight;
- and
- extruding the coagulated polymer from the chamber by way of an exit in the downstream portion of the chamber.