# US 4,086,319 A · Recovery of chromium from tannery waste

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,086,319 A
- Document ID: US4086319A
- Status: Granted
- Kind: A
- Application number: 05/740,016
- Filed: 1976-11-08
- Granted: 1978-04-25
- Earliest claimed: 1976-06-09
- Inventors: Bradford H. Jones
- Web page: https://patentgrep.com/patent/US4086319A

## CPC

- F23G 7/00: Incinerators or other apparatus for consuming industrial waste, e.g. chemicals (incinerator closets A47K11/02; oxidation of sludge C02F11/06; burners in general, burner details F23D; incinerating radioactive waste G21F9/00)
- C14C 3/32: Recovering tanning agents from leather
- Y02W 30/50: Reuse, recycling or recovery technologies
- F23G: CREMATION FURNACES; CONSUMING WASTE PRODUCTS BY COMBUSTION
- C14C: CHEMICAL TREATMENT OF HIDES, SKINS OR LEATHER, e.g. TANNING, IMPREGNATING, FINISHING; APPARATUS THEREFOR; COMPOSITIONS FOR TANNING (bleaching of leather or furs D06L; dyeing of leather or furs D06P)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A process is disclosed for incinerating tannery waste solids containing organic material and chromium which comprises burning at least one ton per day of said waste in the combustion zone of an industrial furnace at a low temperature, preferably between about 800.degree. F. and 1200.degree. F., to convert at least a portion of the organic material to gases and the chromium to ash, removing the gases from the combustion zone and subjecting them to further oxidation, and removing the ash from the furnace. The waste solids include sludge separated from liquid waste, leather scrap, or preferably both. By controlling temperature, waste composition, or both, the chromium in the ash can be obtained in either trivalent or hexavalent form. The hexavalent chromium can be extracted with solvent for reuse in the tanning process. Trivalent chromium, with or without carbon, can be recovered as chromic oxide in an improved stable form for landfill, storage or shipment to a reprocessing center.

## Claims

### Claim 1

The method of processing tannery waste solids containing trivalent chromium and organic material and recovering chromium therefrom, said method comprising:
(a) burning at least one ton per day of said waste in the combustion zone of an industrial furnace at a temperature below about 1200.degree. F. in the presence of sufficient alkali to oxidize the majority of said chromium to hexavalent chromium in the furnace ash and to convert at least a portion of said organic material to gases;
(b) removing said gases from the combustion zone and subjecting them to further oxidation; and,
(c) removing said ash from the furnace and recovering said hexavalent chromium therefrom.

### Claim 2 (depends on 1)

The method according to claim 1 wherein said temperature is between about 800.degree. F. and 1200.degree. F., and said hexavalent chromium is recovered by leaching with a solvent therefor which is inert to trivalent chromic oxide.

### Claim 3 (depends on 2)

The method according to claim 2 wherein said temperature is between about 900.degree. F. and about 1000.degree. F., and wherein more than about 80% of the trivalent chromium in said waste is oxidized to hexavalent chromium in said furnace and recovered.

### Claim 4 (depends on 2)

The method according to claim 2 wherein said waste solids comprise chrome-tanned leather scrap.

### Claim 5 (depends on 4)

The method according to claim 4 wherein a portion of said leather scrap comprises a spend filter body of ground scrap through which tannery waste liquid has been filtered.

### Claim 6 (depends on 2)

The method according to claim 2 wherein said waste solids comprise a chromium containing alkaline sludge separated from liquid tannery waste.

### Claim 7 (depends on 2)

The method according to claim 2 wherein said solvent is an aqueous acid.

### Claim 8 (depends on 7)

The method according to claim 7 wherein said solvent is nitric or sulfuric acid.

### Claim 9 (depends on 2)

The method according to claim 2 wherein at least a portion of said alkali is carbonate.

### Claim 10 (depends on 9)

The method according to claim 9 wherein said tannery waste solids comprise a mixture of carbonate-containing alkaline sludge and chrome-tanned leather scrap.

### Claim 11 (depends on 10)

The method according to claim 10 wherein said mixture contains a proportion of said alkaline sludge sufficient to supply substantially all of said alkali.

### Claim 12 (depends on 1)

The method according to claim 1 comprising the further preliminary steps of separating chromium containing alkaline sludge from tannery liquid waste and partially dewatering said sludge, said tannery waste solids comprising a wet mixture of said sludge and leather scrap having more than about 20% by weight solids.

### Claim 13 (depends on 12)

The method according to claim 12 wherein said leather scrap is added to said sludge prior to dewatering.

### Claim 14 (depends on 1)

The method according to claim 1 wherein said gases are subjected to further heat in an after-burner at a temperature above about 1400.degree. F.

### Claim 15 (depends on 1)

The method according to claim 1 wherein said furnace is a molten salt furnace and said gases are subjected to further oxidation by contact with the hot molten salt, said alkali being admixed with the waste externally of the molten salt.

### Claim 16

The method of disposing of both liquid and solid tannery wastes containing trivalent chromium and organic material to minimize environmental pollution and recover chromium therefrom, said method comprising:
(a) providing in a separation tank a mixture of alkaline beamhouse waste liquids and spent chrome tanning solution;
(b) separating from said liquids an alkaline sludge containing said trivalent chromium; (c) partially dewatering said sludge;
(d) mixing said sludge with scrap chrome-tanned leather, the mixture having at least about 20% by weight solids;
(e) burning at least one ton per day of said mixed solids in the combustion zone of an industrial furnace at a temperature between about 800.degree. F. and about 1200.degree. F. in the presence of sufficient alkali to oxidize the majority of said trivalent chromium to hexavalent chromium in the ash and at least a portion of said organic materials to gases;
(f) removing said gases from the combustion zone and subjecting them to further oxidation; and
(g) recovering said hexavalent chromium from the ash by leaching with a solvent therefor which is inert to trivalent chromic oxide.

### Claim 17 (depends on 16)

The method according to claim 16 comprising the further steps of filtering liquid from said settling tank through a sorptive filter body of ground leather scrap, and burning the spent leather scrap from said filter body in said furnace.

### Claim 18 (depends on 16)

The method according to claim 16 wherein the heat of combustion of said waste supplies substantially all the heat necessary to operate the process after initial heating.

### Claim 19 (depends on 16)

The method according to claim 16 wherein at least a portion of said alkali is carbonate contained in said sludge and substantially all of said trivalent chromium is oxidized in the furnace and recovered.