Abstract
Polymeric phosphine oxides having the formula ##STR1## WHERE R is an alkyl group of from 1 to 20 carbon atoms, or an aryl group of from 6 to 20 carbon atoms, R' is a phenylene or naphthylene group, and n is from 2 to 50 or preferably 5 to 25. The invention also relates to compositions of such polymeric phosphine oxides with organic polymers such as polyesters, e.g. ethylene terephthalate and polyamides, e.g. hexamethylene adipamide. The combination of the present polymeric phosphine oxides with the organic polymers makes it possible to obtain flame retardant products useful in many applications such as for carpeting and clothing.
Claims9
The combination of an organic polymer together with a polyphosphine oxide corresponding to the formula ##STR20## an alkyl group of 1 to 20 carbon atoms or an aryl group of 6 to 20 carbon atoms, R' is a phenylene or naphthylene group, and n is from 2 to 50 units.
The combination of an organic polymer together with a polyphosphine oxide corresponding to the formula ##STR21## phenylene group, R is a methyl group, and n is from 2 to 50 units.
The combination of an organic polymer together with a polyphosphine oxide corresponding to the formula ##STR22## naphthylene group, R is an alkyl group of 1 to 20 carbon atoms or an aryl group of 6 to 20 carbon atoms, and n is from 2 to 50 units.
The combination of polyethylene terephthalate together with a polyphosphine oxide corresponding to the formula ##STR23## phenylene group, R is a methyl group, and n is from 2 to 50 units.
The combination of polyethylene terephthalate together with a polyphosphine oxide corresponding to the formula ##STR24## naphthylene group, R is an alkyl group of 1 to 20 carbon atoms or an aryl group of 6 to 20 carbon atoms, and n is from 2 to 50 units.
The combination of a polyamide resin together with a polyphosphine oxide corresponding to the formula ##STR25## phenylene group, R is a methyl group, and n is from 2 to 50 units.
The combination of polyamide resin together with a polyphosphine oxide corresponding to the formula ##STR26## naphthylene group, R is an alkyl group of 1 to 20 carbon atoms or an aryl group of 6 to 20 carbon atoms, and n is from 2 to 50 units.
Process for improving the flame retardancy properties of an organic polymer which comprises combining the said organic polymer with a polyphosphine oxide corresponding to the formula ##STR27## phenylene or naphthylene group, R is an alkyl group of 1 to 20 carbon atoms or an aryl group of 6 to 20 carbon atoms, and n is from 2 to 50 units.
Process for preparing polyphosphine oxides corresponding to the formula ##STR28## phenyl or naphthyl group, R is an alkyl group of 1 to 20 carbon atoms or an aryl group of 6 to 20 carbon atoms, and n is from 2 to 50 units, which comprises dehaloalkylating in the presence of a nickel compound at a temperature of 50.degree. C to 300.degree. C a monomeric compound having the general formula ##STR29## where X is chlorine or bromine, R is an alkyl group of 1 to 20 carbon atoms, or an aryl group of 6 to 20 carbon atoms, R' is phenylene or naphthylene and R" is an alkyl group of 1 to 20 carbon atoms.
Dependencies are inferred from the claim text.