Method of cleaning raw ore
OwnerWilliam Benzoninventor
Life of this patent
Estimating the term…
Abstract
A method of cleaning a raw ore product such as coal is disclosed wherein the ore product temperature is increased up to about 200.degree.-212.degree. F. before water is separated therefrom whereby the moisture content of the cleaned product is controlled. The ore product is passed through a bath of hot water, then surface water is removed before the ore product is moved through an evaporative cooler in a downward direction while being subjected to air at ambient temperature and at an air capacity of between 10,000 and 15,000 cubic feet per ton of ore product.
Claims7
A method of cleaning a raw ore product such as coal comprising the steps of heating the ore product by conveying the ore product through a bath of hot water, then removing surface water from the ore product, and then drying the ore product to the desired moisture content by use of an evaporative cooler, said ore product moving through said evaporative cooler in a downward direction while being contacted by moving air traveling in a transverse direction, said air moving at a rate of substantially between 10,000 and 15,000 cubic feet per ton of ore product.
A method of cleaning raw ore products comprising the steps of subjecting the raw ore products to a rinse screen wherein the ore products are divided into two flow paths based on the size of the screen, heating the large sized ore products by conveying them through a bath of hot water, and then removing surface water from the heated larger sized ore products, then drying the said heated larger sized ore product to the desired moisture content by use of an evaporative cooler, said drying of the larger sized ore products occurring while the ore products are moving downwardly through the evaporative cooler and are being subjected to air at ambient temperature wherein the air capacity is substantially between 10,000 and 15,000 cubic feet per ton of the larger sized ore product, removing tailings from the smaller sized ore products, then heating the smaller sized ore products to a temperature less than about 212.degree. F., and then drying the smaller size ore products to a moisture content greater than the moisture content of the dried larger sized ore products.
Dependencies are inferred from the claim text.