The invention relates to a method for preparation of cationactive and amphoteric ion-exchangers from non-ionogenic crosslinked copolymers containing hydroxyl groups by their reaction with mineral acids, addition products of sulfur trioxide, sulfuric acid or chlorosulfuric acid with alcohols or pyridine, unsaturated compounds, as acrylonitrile, methacrylonitrile or sodium vinylsulfonate in a strongly alkaline medium, or with halogenoalkylammonium compounds. The starting copolymer containing hydroxyl groups is prepared by the suspension copolymerization of monomers, selected from the group which comprises hydroxyalkyl methacrylates and acrylates and oligoglycol acrylates and methacrylates, with crosslinking divinyl monomers, e.g. divinylbenzene, ethylene dimethacrylate, butylenediol dimethacrylate or diacrylate, and advantageously has the macroporous structure. The products are suitable for application in column process thanks to their favorable mechanical properties, namely for chromatographic separation of hydrophilic compounds, e.g. biological materials as aminoacids. The hydrophilicity of the product may be varied by selection of monomers for the starting copolymer, by the type of ionactive substitution and by the degree of transformation.
A method for preparation of cationactive ion-exchangers from macroporous hydrophilic polymers containing crosslinked copolymers having hydroxyl groups in their structure, said crosslinked copolymers being prepared by suspension copolymerization of monomers selected from the group consisting by hydroxyalkyl methacrylates, hydroxyalkyl acrylates, oligoglycol acrylates and oligoglycol methacrylates, with crosslinking divinyl monomers selected from the group consisting of divinylbenzene, ethylene dimethacrylate, butylenediol diacrylate, said copolymers being modified by treatment with a material selected from the group consisting of sulfuric acid, chlorosulfuric acid - pyridine complex and metaphosphoric acid - alcohol complexes at a temperature of 20.degree. - 50.degree. C. for 0.4 - 40 hours.
Dependencies are inferred from the claim text.