# US 4,065,297 A · Process for dephosphorizing molten pig iron

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,065,297 A
- Document ID: US4065297A
- Status: Granted
- Kind: A
- Application number: 05/756,968
- Filed: 1977-01-04
- Granted: 1977-12-27
- Earliest claimed: 1976-09-28
- Assignees: Sumitomo Metal Industries, Ltd.
- Inventors: Kantaro Sasaki; Takami Ikeda; Tohru Matsuo; Takashi Okazaki
- Web page: https://patentgrep.com/patent/US4065297A

## CPC

- C21C 1/02: Dephosphorising or desulfurising
- C21C: PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS

## Abstract

A process for dephosphorizing molten pig iron by adding (a) lime, converter slag and/or iron oxide, (b) iron oxide and/or oxidizing gas, and if necessary (c) flourspar and/or soda ash to the molten pig iron stored in a treating vessel in order to adjust the amount of % CaO to correspond to 0.3 to 3.0 times the sum of the amounts of % SiO.sub.2 and % P.sub.2 O.sub.5 and to adjust the amount of total iron to 15 to 50%, in the slag composition after treatment, thereby obtaining a high dephosphorization.

## Claims

### Claim 1

A process for dephosphorizing molten pig iron prior to charging it into a converter so as to obtain pig iron having a low phosphorus content, the process including
1. forming a slag by
a. adding a dephosphorizing agent to the molten pig iron when the pig iron is at a temperature of less than 1450.degree. C;
b. adding an oxidizing agent to the molten pig iron when the pig iron is at a temperature of less than 1450.degree. C; and
2. removing the slag;
said steps (1) (a) and (1) (b) being such as to form a slag having a % CaO in an amount which corresponds to 0.3 to 3.0 times the sum of the amounts of % SiO.sub.2 and % P.sub.2 O.sub.5, and a total iron of 15 to 50%.

### Claim 2 (depends on 1)

A process according to claim 1, wherein said added dephosphorizing agent is selected from the group consisting of iron oxide, converter slag, limestone and lime.

### Claim 3 (depends on 1)

The process according to claim 1, wherein said added oxidizing agent is selected from the group consisting of iron oxide, oxygen gas and mixtures thereof.

### Claim 4 (depends on 1)

The process according to claim 1, wherein in forming said slag a further step (1) (c) of adding at least one slagging promoter to the molten pig iron is included.

### Claim 5 (depends on 4)

The process according to claim 4, wherein said added at least one slagging promoter is selected from the group consisting of fluorspar and soda ash.

### Claim 6 (depends on 4)

The process according to claim 4, wherein said slagging promoter is added to said molten pig iron in an amount up to 15kg per ton of pig iron.

### Claim 7 (depends on 1)

The process according to claim 1, wherein said oxidizing agent is added to said pig iron in an amount which oxidizes all the Si, Mn and P contained in said pig iron but no more than 1.5 wt.% of the carbon.

### Claim 8 (depends on 1)

The process according to claim 1, wherein said oxidizing agent is an oxidizing gas which is added to said molten pig iron by passage through an immersion pipe.

### Claim 9 (depends on 1)

The process according to claim 1, wherein said oxidizing agent is an oxidizing gas which is added to said molten pig iron by being blown onto the surface of the molten pig iron by a lance.

### Claim 10 (depends on 1)

The process according to claim 1, wherein said dephosphorizing agent and said oxidizing agent are added to said molten pig iron while said molten pig iron is stirred by bubbling an inert gas therethrough.

### Claim 11 (depends on 1)

The process according to claim 1, wherein said dephosphorizing agent and said oxidizing agent are added to said molten pig iron while said molten pig iron is stirred by an impeller.