Cosmetic oil containing isobutylene
AssigneeNichiyu Kagaku Co., Ltd.
InventorsMoritoshi Yoshida, Takashi Yamamoto, Sumito Nii
Life of this patent
Estimating the term…
Abstract
Polymers of C4 olefins having a viscosity of 15 to 35 centistokes at 100.degree. F show improved performance as cosmetic oils, in comparison with squalane. These polymers are prepared by polymerizing (a) isobutylene by itself, or (b) C4 hydrocarbon olefin containing a mixture of at least two of isobutylene, 1-butene, 2-butene and butadiene, using a catalyst; then removing high molecular weight and low molecular weight compounds by distillation; hydrogenating the remainder of the polymerization product; removing carbonyl compounds therefrom if necessary and further purifying the resultant polymer by steam distillation or treating same with activated carbon or solvent extraction, to deodorize same.
Claims2
An oil-based cosmetic composition containing from 3 to 50 percent by weight of a cosmetic oil and the balance is conventional cosmetic ingredients for oil-based cosmetic compositions, said cosmetic oil having been prepared by polymerizing a substance consisting essentially of isobutylene or a mixture of isobutylene and one or more olefins selected from the group consisting of 1-butene, 2-butene, 1,2-butadiene and 1,3-butadiene, at a temperature of from -30.degree. to +60.degree. C, in the presence of a Friedel-Craft's catalyst or Lewis acid, to obtain a crude liquid polymer product;
- distilling said crude liquid polymer product under reduced pressure to separate materials having boiling points of less than 120.degree. C at 1 to 2 mmHg and materials having boiling points of more than 200.degree. C at 1 to 2 mmHg, and recovering a purified polymer product having a boiling point range of from 120.degree. to 200.degree. C at 1 to 2 mmHg and having an average molecular weight in the range of from about 250 to about 600;
- hydrogenating said purified polymer product to hydrogenate substantially all the double bonds in said purified polymer product;
- and deodorizing said hydrogenated purified polymer product to obtain said cosmetic oil by one of the steps of (1) steam distilling the hydrogenated purified polymer product under reduced pressure at a temperature below 130.degree. C, or (2) treating the hydrogenated purified polymer product with activated carbon, or (3) effecting solvent extraction of the hydrogenated purified polymer product, or combinations of steps (1), (2) and (3), to remove impurities from the hydrogenated purified polymer product, said cosmetic oil having an average molecular weight in the range of from 250 to 600 and being substantially free of materials having molecular weights below 250 and above 600, said cosmetic oil being colorless and odorless, having a peroxide value, a bromine number, a carbonyl value and an acid value all of substantially zero, and having a viscosity of from 15 to 35 centistokes at 100.degree. F.
Dependencies are inferred from the claim text.