# US 4,060,423 A · High-temperature glass composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,060,423 A
- Document ID: US4060423A
- Status: Granted
- Kind: A
- Application number: 05/708,949
- Filed: 1976-07-27
- Granted: 1977-11-29
- Earliest claimed: 1976-07-27
- Assignees: General Electric Company
- Inventors: George L. Thomas
- Web page: https://patentgrep.com/patent/US4060423A

## CPC

- H01K 1/38: Seals for leading-in conductors
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 8/24: Fusion seal compositions being frit compositions having non-frit additions, i.e. for use as seals between dissimilar materials, e.g. glass and metal; Glass solders
- C03C 27/02: by fusing glass directly to metal
- Y10T 428/294: including metal or compound thereof [excluding glass, ceramic and asbestos]
- H01K: ELECTRIC INCANDESCENT LAMPS (details, apparatus or processes for manufacture applicable to both discharge devices and incandescent lamps H01J; light sources using a combination of incandescent and other types of light generation H01J61/96, H05B35/00)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Aluminosilicate glasses containing BaO and CaO are provided having combined high softening points along with exceptionally low liquidus temperatures. These glasses are within the following compositional limits in percent by weight: ______________________________________ Percentage Oxides Range ______________________________________ SiO.sub.2 55-68 Al.sub.2 O.sub.3 15-18 CaO 7-13 BaO 6-16 ______________________________________ except for incidental impurities, residual fluxes and refining agents. The weight ratio of Al.sub.2 O.sub.3 to combined weight ratio of CaO and BaO in the present glass composition is maintained in the range 0.6:1 to 1:1. Such glasses provide an improved hermetic seal for high temperature lamp envelopes.

## Claims

### Claim 1

A molybdenum seal glass composition which consists essentially of oxides in approximate percent by weight 55-68 SiO.sub.2, 15-18 Al.sub.2 O.sub.3, 7-13 CaO, and 6-16 BaO, along with minor amounts of incidental impurities, residual fluxes, and refining agents, wherein the weight ratio of Al.sub.2 O.sub.3 to combined weight ratio of CaO and BaO is about in the range 0.6:1 to 1:1 so as to reside in the eutectic region of this aluminosilicate system, said glass composition having a liquidus temperature no greater than about 1250.degree. C, a strain point of at least about 725.degree. C, and an average coefficient of linear thermal expansion in the 0-300.degree. C temperature range between about 42 .times. 10.sup.-7 cm/cm/.degree. C to about 48 .times. 10.sup.-7 cm/cm/.degree. C.

### Claim 2 (depends on 1)

A glass composition as in claim 1 which is essentially alkali metal ion free and lead oxide free.

### Claim 3 (depends on 1)

A glass composition as in claim 1 wherein the mole % CaO content exceeds the mole % BaO content.

### Claim 4

A molybdenum seal glass composition for a regenerative cycle halogen-containing incandescent lamp which consists essentially of oxides in approximate percent by weight 63 SiO.sub.2, 16 Al.sub.2 O.sub.3, 9 CaO, and 12 BaO so as to reside in the eutectic region of this aluminosilicate system, along with minor amounts of incidental impurities, residual fluxes and refining agents, said glass composition having a liquidus temperature of approximately 1200.degree. C, an average coefficient of linear thermal expansion in the 0.degree.-300.degree. C temperature range of about 43.5 .times. 10.sup.-7 cm/cm/.degree. C, and a strain point of at least 750.degree. C.