This disclosure deals with novel very fine, particulated colloidal platinum of the 15-25 Angstrom size range of unusual catalytic activity and particularly adapted for adsorption upon various substrata, and produced from a new platinum sulfite acid and a sol derived therefrom, with novel methods of preparation thereof being disclosed.
Claims9
A method of forming a platinum colloid sol of finely divided particles of average size of substantially 15-25 Angstroms, that comprises, oxidizing, by heating in air to dryness, a complex sulfite acid represented substantially by the empirical formula H.sub.3 Pt(SO.sub.3).sub.2 OH to produce a black, glossy, oxidized material, and dispersing said glossy material in water.
A method of forming a platinum colloid sol of finely divided particles of average size of substantially 15-25 Angstroms, that comprises, adding sodium bisulfite to a substantially neutral solution of sodium chloroplatinate until the pH drops to at least about 4, adding sodium carbonate to bring the pH back to substantially 7 thereby precipitating a complex sodium platinum sulfite salt containing substantially six atoms of sodium and four moles of sulfite per atom of platinum, subjecting said precipiate to strong hydrogen-form ion exchange resin to exchange six atoms of sodium with hydrogen and to liberate substantially two moles of sulfite per atom of platinum thereby producing a solution of a complex platinum sulfite acid comprising substantially two moles of sulfite per atom of platinum, concentrating said complex platinum sulfite acid solution, oxidizing said complex acid by heating the same to dryness in air to produce a black, glossy, oxidized material, and dispersing said glossy material in water.
A method of forming a platinum colloid sol of finely divided particles of average size of substantially 15-25 Angstroms, that comprises, subjecting a complex platinum sulfite salt containing substantially six atoms of sodium and four mols of sulfite per atom of platinum to strong hydrogen-form ion exchange resin to exchange six atoms of sodium with hydrogen and to liberate substantially two moles of sulfite per atom of platinum thereby producing a solution of a complex platinum sulfite acid comprising substantially two moles of sulfite per atom of platinum, concentrating said complex platinum sulfite acid solution, oxidizing said complex acid by heating the same to dryness in air to produce a black, glossy, oxidized material, and dispersing said glossy material in water.
A platinum colloidal sol consisting essentially of black, glossy, oxidized complex platinum sulfite acid dispersed in water, said oxidized acid being in the form of finely divided particles of average size of substantially 15-25 Angstroms.