Abstract
In trivalent chromium electroplating baths of the type which comprise an aqueous solution of a complex of trivalent chromium with a carboxylic acid such as a glycolic acid and a halide such as a chloride, the invention provides an improvement by adding ammonia to the baths in a proportion of at least 0.05 moles per liter, thereby obtaining substantially improved covering power.
Claims5
An aqueous chromium electroplating bath having a pH between 1.8 and 4.9 consisting essentially of water, from 0.05 moles to saturation of ammonia and a water soluble complex of trivalent chromium with (A) glycolic acid, and (B) 0.1 to 3.5 moles of a halide per mole of chromium, said chromium being present in an amount sufficient to provide 0.5 to 3 moles per liter of trivalent chromium.
An aqueous chromium electroplating bath having a pH of from 1.8 to 4.9 and consisting essentially of water, from 0.2 to 4 molar ammonium, from 1 to 5 molar of at least one salt selected from the chlorides and sulphates of sodium and potassium and a complex of trivalent chromium with (A) from 0.7 to 3 moles of glycolic acid per mole of chromium and (B) from 0.1 to 1 mole of chloride per mole of trivalent chromium.
Dependencies are inferred from the claim text.