# US 4,050,052 A · Electrical temperature measuring resistor structure, particularly for resistance thermometers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,050,052 A
- Document ID: US4050052A
- Status: Granted
- Kind: A
- Application number: 05/695,783
- Filed: 1976-06-14
- Granted: 1977-09-20
- Earliest claimed: 1975-06-21
- Assignees: W. C. Heraeus GmbH
- Inventors: Walter Reichelt; Gunter Sauer
- Web page: https://patentgrep.com/patent/US4050052A

## CPC

- G01K 7/18: the element being a linear resistance, e.g. platinum resistance thermometer (G01K7/26 takes precedence)
- H01C 7/22: Elongated resistive element being bent or curved, e.g. sinusoidal, helical
- H01C 17/08: by vapour deposition
- H01C 17/12: by sputtering
- G01K: MEASURING TEMPERATURE; MEASURING QUANTITY OF HEAT; THERMALLY-SENSITIVE ELEMENTS NOT OTHERWISE PROVIDED FOR (radiation pyrometry G01J5/00)
- H01C: RESISTORS

## Abstract

A substrate carrier of electrically non-conductive material has a strip of resistance platinum applied thereto; in order to avoid the use of an intermediate temperature coefficient of expansion matching layer, the substrate carrier, for example of aluminum oxide, beryllium oxide, or a magnesium silicate, has less than thirty parts per million (ppm) Fe, less than 15 ppm Cr, less than 45 ppm Pb and less than 70 ppm Si in a form capable of reacting with platinum, the sum of the impurities by these metals, if all, or more than one are present, not exceeding 20 ppm; the average thermal coefficient of expansion of the substrate does not deviate from the mean thermal coefficient of expansion of the thermometer grade platinum by more than .+-. 30%; the platinum layer has a thickness of from 0.1 to 10 .mu.m, and is applied at a temperature in the range of between about 1000.degree. C to 1400.degree. C during 60 minutes in an atmosphere containing oxygen, for example free air.

## Claims

### Claim 1

Electrical measuring resistor structure for use in resistance thermometers having
a carrier (1) of electrically non-conductive material and a strip of platinum resistance layer (2) applied to the carrier in a predetermined pattern, and comprising the improvement wherein
the carrier comprises a substrate (1) which includes less than 30 parts per million (ppm) Fe, less than 15 ppm Cr, less than 45 ppm Pb and less than 70 ppm Si in a form which can react with the platinum and wherein the sum of said named materials, if more than one is present, does not exceed 20 ppm;
the platinum layer has a thickness of between 0.1 and 10 .mu.m;
and the mean thermal coefficient of expansion of the substrate differs from the coefficient of expansion of the thermal platinum by less than about .+-. 30%.

### Claim 2 (depends on 1)

Structure according to claim 1, wherein the substrate comprises at least one of: aluminum oxide, beryllium oxide, thorium oxide, magnesium oxide, a magnesium silicate.

### Claim 3 (depends on 1)

Structure according to claim 1, further comprising a cover layer (3) for protection of the strip of platinum (2) and the substrate, said cover being high temperature and mechanical wear resistant.

### Claim 4 (depends on 3)

Structure according to claim 3, wherein the cover layer (3) comprises metal oxides of at least one: aluminum, beryllium, thorium, rare earths.

### Claim 5 (depends on 1)

Structure according to claim 1, wherein the substrate comprises aluminum oxide.

### Claim 6 (depends on 1)

Structure according to claim 1, wherein the platinum layer has a thickness of between 1 to 5 .mu. m.

### Claim 7 (depends on 1)

Structure according to claim 1, wherein the substrate (1) with the strip of platinum (2) applied, is heated in an oxygen-containing atmosphere to a temperature in the range of between about 1000.degree. to 1400.degree. C. for a period of at least 60 minutes.

### Claim 8 (depends on 1)

Structure according to claim 1, wherein the substrate (1) during application of the strip (2) of platinum is at a temperature in the range of about between 500.degree. to 900.degree. C.

### Claim 9 (depends on 1)

Structure according to claim 1, wherein the substrate (1) before application of the strip (2) of platinum is heat-treated in air.

### Claim 10 (depends on 1)

Structure according to claim 1, wherein the substrate (1) with the strip (2) of platinum applied thereto is heated in air to a temperature of between about 1050.degree. to about 1150.degree. C. for a period of about 3 hours.

### Claim 11 (depends on 2)

Structure according to claim 2, further comprising a metal oxide cover layer (3) including at least one of: aluminum oxide, beryllium oxide, thorium oxide, an oxide of a rare earth; the platinum strip (2) has a thickness of between 1 to 5 .mu.m, and the substrate (1) with the strip of platinum (2) applied thereto is heated in air to a temperature of between about 1050.degree. to 1150.degree. C. for a period of about 3 hours.

### Claim 12 (depends on 11)

Structure according to claim 11, wherein the substrate comprises aluminum oxide.

### Claim 13

Method to make a resistor structure, particularly for resistance thermometers
having a substrate (1) which includes less than 30 parts per million (ppm) Fe, less than 15 ppm Cr, less than 45 ppm Pb and less than 70 ppm Si in a form which can react with the platinum and wherein the sum of said named materials, if more than one is present, does not exceed 20 ppm;
the platinum layer has a thickness of between 0.1 and 10 .mu.m;
and the mean thermal coefficient of expansion of the substrate differs from the coefficient of expansion of the thermal platinum by less than about .+-.30%;
and wherein the substrate (1) with the strip of platinum (2) applied thereto is heated to a temperature in the range of about 1000.degree. to 1400.degree. C. in an atmosphere containing oxygen for about 1 hour.

### Claim 14 (depends on 13)

Method according to claim 13, wherein the substrate, during deposition of the strip of platinum (2) has a temperature in the range of about 500.degree. to 900.degree. C.

### Claim 15 (depends on 14)

Method according to claim 14, wherein the strip of platinum is applied by vapor deposition by means of electron beam heating.

### Claim 16 (depends on 13)

Method according to claim 13, further comprising the step of heat-treating the substrate (1) before application of the strip of platinum (2) thereto in air.

### Claim 17 (depends on 15)

Method according to claim 15, wherein the platinum strip (2) has a thickness of between 1 to 5 .mu. and the substrate (1) with the strip of platinum applied thereto is heated in air to a temperature of between about 1050.degree. to 1150.degree. C. for a period of time of about 3 hours.