Abstract
Improved melt blending process for preparing block copolymer of poly(4,7-dioxadecamethylene adipamide)-polycaprolactam, which is also known as N-30203-6//6, involves continuing the melt blending until the polymer is characterized in that the maximum amount of the block copolymer recovered from an aqueous formic acid solution containing the dissolved block copolymer exceeds about 90%. Fiber prepared from such a characterized block copolymer does not fuse when scoured in boiling water.
Claims3
In the process of melt-blending poly(4,7-dioxadecamethylene adipamide) and polycaprolactam wherein the improvement comprises continuing the melt blending until the clock copolymer is characterized in that the maximum amount of block copolymer recovered from an aqueous formic acid solution containing the dissolved block copolymer exceeds about 90.6 weight %.
In the process of melt-blending poly(4,7-dioxadecamethylene adipamide) and polycaprolactam wherein the improvement comprises continuing the melt blending until the block copolymer is characterized in that the formic acid concentration is less than about 52.5% at 50% recovery of the block copolymer dissolved in an aqueous formic acid solution containing the dissolved block copolymer.
Dependencies are inferred from the claim text.