# US 4,031,184 A · Process for reclaiming cement kiln dust and recovering chemical values therefrom

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,031,184 A
- Document ID: US4031184A
- Status: Granted
- Kind: A
- Application number: 05/649,064
- Filed: 1976-01-14
- Granted: 1977-06-21
- Earliest claimed: 1976-01-14
- Assignees: Donald L. Christensen
- Inventors: Andrew T. McCord
- Web page: https://patentgrep.com/patent/US4031184A

## CPC

- C01D 3/08: Preparation by working up natural or industrial salt mixtures or siliceous minerals
- C01D: COMPOUNDS OF ALKALI METALS, i.e. LITHIUM, SODIUM, POTASSIUM, RUBIDIUM, CAESIUM, OR FRANCIUM (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides C01B17/22; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia and cyanogen, containing nitrogen and other non-metals C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; phosphides C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20)

## Abstract

This invention relates to a process of reclaiming cement kiln dust and recovering the alkali content thereof which comprises leaching the cement kiln dust at elevated temperatures with an aqueous solution of potassium chloride, treating the leached slurry of cement kiln dust with a relatively small amount of oil and a fatty acid to flocculate, and preferably pelletize, the solids, in the aqueous phase, extracting the flocculated or pelletized dust from the aqueous phase, desirably lightly washing or rinsing the flocculated or pelletized material to still further reduce the alkali content, cooling the leaching solution to throw down or precipitate potassium chloride crystals by crystallization, and removing the crystallized material therefrom. The residual leaching solution, after removal of substantial amounts of potassium chloride crystals, is still saturated with potassium chloride in solution, and after reheating is available for recycling with additional cement kiln dust.

## Claims

### Claim 1

A process for reclaiming cement kiln dust in usable form and recovering the alkali values thereof comprising leaching the cement kiln dust at an elevated temperature with an aqueous solution of potassium chloride, treating the leached slurry of cement kiln dust with a relatively small amount of oily hydrocarbon in the order of 1% to 10% by weight based on the weight of solids in the slurry and a long chain fatty acid amounting to at least 0.1% by weight based on the weight of the added oily hydrocarbon to flocculate the solids in an aqueous phase, separating the solids, cooling the resulting aqueous phase to crystallize potassium chloride out of solution, and separating the crystallized potassium chloride from the solution.

### Claim 2 (depends on 1)

A process according to claim 1 in which the flocculated dust, after separation from the aqueous phase, is lightly washed with water to further remove any residual potassium chloride.

### Claim 3 (depends on 1)

A process according to claim 1 in which the leaching is carried out at a temperature of 70.degree. to 80.degree. C.

### Claim 4 (depends on 1)

A process according to claim 1 in which the leaching solution, after extraction of the flocculated cement dust, is cooled to 10.degree. to 20.degree. C. to crystallize out potassium chloride.

### Claim 5 (depends on 1)

A process according to claim 1 in which the leaching solution, after removal of the crystallized potassium chloride, is reheated and recycled for the leaching of additional cement kiln dust.

### Claim 6 (depends on 1)

A process according to claim 1 in which the leaching solution contains a sufficient amount of calcium chloride to convert any insoluble salts of potassium contained in the cement kiln dust to soluble potassium chloride.

### Claim 7 (depends on 1)

A process according to claim 1 in which the leaching solution contains a sufficient amount of HCl to convert any insoluble salts of potassium contained in the cement kiln dust to soluble potassium chloride.

### Claim 8 (depends on 1)

A process according to claim 1 in which the amount of oil used to flocculate the cement dust slurry is in the order of 1% by weight based on the weight of the solids content of the slurry.

### Claim 9

A process for reclaiming cement kiln dust in usable form and recovering the alkali values thereof comprising leaching the cement kiln dust at an elevated temperature with an aqueous solution of potassium chloride, treating the leached slurry of cement kiln dust with a relatively small amount of oily hydrocarbon in the order of 1 to 10% by weight based on the weight of solids in the slurry and a long chain fatty acid amounting to at least 0.1% by weight based on the weight of the added oily hydrocarbon to flocculate the solids, and agitating to pelletize the solids in an aqueous phase, extracting the pelletized solids from the aqueous phase, cooling the resulting aqueous phase to crystallize potassium chloride out of solution, and separating the crystallized potassium chloride from the solution.

### Claim 10 (depends on 9)

A process according to claim 9 in which the amount of oil used to pelletize the cement dust slurry is in the order of about 5% by weight based on the weight of the solids content of the slurry.