Process for defluorination of commercial phosphoric acid
AssigneeAtlantic Richfield Company
InventorEverett N. Case
Life of this patent
Estimating the term…
Abstract
A process is provided for the defluorination of wet process phosphoric acid whereby hydrogen ion is removed, and the concentration of P.sub.2 O.sub.5 is adjusted with water, the calcium concentration, calculated as CaO, is adjusted by adding a source of calcium phosphate at temperatures of about 25.degree. C. to 75.degree. C. while maintaining a pH of about 2 or below to achieve substantially the maximum calcium content in aqueous solution and raising the temperature of the solution to about the boiling point to initiate the hydrolysis of silicofluoride and precipitate calcium fluoride which is separated, thereby producing a solution with an enhanced phosphoric acid content.
Claims15
A process for the defluorination of wet process phosphoric acid containing sulfate ions and fluosilicate ions which comprises adding to the phosphoric acid a calcium phosphate thereby precipitating calcium sulfate and forming an acid solution having an increased Ca.sup.+.sup.+ ion and P.sub.2 O.sub.5 concentration, diluting said acid solution with water to adjust the P.sub.2 O.sub.5 concentration to within a range of about 18 to 32 percent P.sub.2 O.sub.5, adjusting the calcium concentration, calculated as CaO, by adding a calcium phosphate at about 25.degree. C. to 75.degree. C. to achieve substantially the maximum calcium content in the solution while maintaining a pH of the acid solution at about 2 or below, raising the temperature of said solution to about the boiling point and maintaining the P.sub.2 O.sub.5 concentration by dilution with water to within the 18 to 32 percent P.sub.2 O.sub.5 range and maintaining said solution at the boiling point to effect the precipitation of calcium fluoride, separating the precipitated calcium fluoride from said solution leaving an acid solution having an increase in total free phosphoric acid as compared to the diluted acid solution prior to heating.
A process for the defluorination of wet process phosphoric acid containing sulfate ions and fluosilicate ions and having about a 30 to 32 percent P.sub.2 O.sub.5 content which comprises the steps of:
- (a) adding phosphate rock to the wet process phosphoric acid to precipitate calcium sulfate;
- (b) removing the precipitated calcium sulfate leaving an acid solution having an increased Ca.sup.+.sup.+ ion and an increased P.sub.2 O.sub.5 concentration;
- (c) adjusting the concentration of P.sub.2 O.sub.5 of the acid solution to about 18 to 32 percent P.sub.2 O.sub.5 by diluting said acid solution with water or a dilute phosphoric acid solution;
- (d) adding phosphate rock at ambient temperature to the diluted acid solution to adjust the calcium concentration and achieve substantially the maximum calcium content, expressed as calcium oxide, while maintaining the pH of the acid solution between about 1 and 2;
- (e) raising the temperature of the solution to within a range of about 90.degree. C. to 110.degree. C. and maintaining the P.sub.2 O.sub.5 concentration to within about 18 to 32 percent P.sub.2 O.sub.5 by dilution with water;
- (f) maintaining the solution at a temperature within a range of about 90.degree. C. to 110.degree. C. to precipitate a calcium fluoride substantially free of silica;
- and
- (g) removing the precipitated calcium fluoride and recovering the defluorinated phosphoric acid.
Dependencies are inferred from the claim text.