# US 4,022,749 A · Formation of composite particulate material using high energy rotary impact milling

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 4,022,749 A
- Document ID: US4022749A
- Status: Granted
- Kind: A
- Application number: 05/556,401
- Filed: 1975-03-07
- Granted: 1977-05-10
- Earliest claimed: 1964-05-18
- Assignees: Entoleter, Inc.
- Inventors: William L. Kuechler
- Web page: https://patentgrep.com/patent/US4022749A

## CPC

- C08K 7/12: Asbestos
- B02C 13/18: with beaters rigidly connected to the rotor
- B29B 7/885: {with means for treating, e.g. milling, the charges (B29B7/905 takes precedence)}
- B29B 13/10: by grinding, e.g. by triturating; by sieving; by filtering
- C08L 23/10: Homopolymers or copolymers of propene
- C08L 23/06: Polyethylene
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08L 83/02: Polysilicates
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2207/14: Amorphous or atactic polypropylene
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- B02C: CRUSHING, PULVERISING, OR DISINTEGRATING IN GENERAL; MILLING GRAIN ({household tools and machines for pulverising foodstuffs, e.g. coffee and spice mills A47J42/00; pharmaceutical mortars A61J3/02; mechanical processing of refuse and garbage B03B9/06; dressing mould materials by grinding B22C5/04}; obtaining metallic powder by crushing, grinding or milling B22F9/04; {recovery of plastics by disintegrating B29B17/00; crushing raw materials in starch making C08B30/02; beaters for papermaking D21D1/02; crushing devices specially for transport in mines E21F13/002; slag crushing devices F23J1/00; fuel milling devices in combustion apparatus F23K1/00; household devices for crushing coal F24B15/02; ice disintegrating devices F25C5/02})
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The formation of composite materials is disclosed, using high energy rotary impact milling. The illustrations utilize polymer resin particles as the matrix material, and solid particle fillers. Ultra-small particle sizes are used for both the matrix and filler materials. When the resultant materials are processed by usual forming techniques, the resultant composite materials possess strength properties approximately equivalent to those of the unfilled matrix material, even though heavily filled.

## Claims

### Claim 1

A method of forming a composite particulate material having a plastic, particulate, integratable ingredient capable of being formed into a continuous phase, coherent body and a particulate additive ingredient of submicro particle size, comprising impact milling of said two ingredients in a rotary mill at a linear speed for the impactors of the mill of at least about 300 feed per second to cause the additive particles to deagglomerate and adhere to the plastic particles as substantially nonagglomerated individual particles until at least about twenty percent of weight of the composite is said additive.

### Claim 2 (depends on 1)

A method as set forth in claim 1, wherein said percentage is at least about 50.

### Claim 3 (depends on 1)

A method as set forth in claim 1, wherein said plastic ingredient comprises polypropylene or polyethylene.

### Claim 4 (depends on 1)

A method as set forth in claim 1, and including applying a higher level of additional energy to the particles incrementally, said additional energy causing said additive particles to adhere tenaciously with said plastic material.

### Claim 5 (depends on 4)

A method as set forth in claim 4, wherein said additional energy is applied to the material by impact milling the material in a rotary impact mill.

### Claim 6 (depends on 5)

A method as set forth in claim 5, wherein said additional energy is obtained by imparting a rotary speed to said mill so as to provide a linear speed to the impactors of the mill of at least about 600 feet per second.

### Claim 7 (depends on 6)

A method as set forth in claim 6, wherein said plastic ingredient is polypropylene or polyethylene.

### Claim 8 (depends on 4)

A method as set forth in claim 4, wherein said additional energy is applied to the material by extrusion of the material.

### Claim 9 (depends on 1)

A method as set forth in claim 1, wherein the impactors attain a linear speed substantially in excess of 300 feet per second.

### Claim 10 (depends on 1)

A method as set forth in claim 1, wherein the linear speed of said impactors is at least about 600 feet per second.

### Claim 11

A method of forming a composite material from a first particulate ingredient capable of being formed into a continuous phase coherent plastic body, and a second particulate ingredient of submicro particle size, said submicro particles having a tendency to cohere into agglomerates, comprising impact milling said two ingredients together by suspending them in a rotary impact mill, and driving said mill at an impactor speed that is sufficient to cause a mix of said two particulate ingredients with a dispersion of said second particulate ingredient throughout said mix and to cause said second ingredient particles to deagglomerate and adhere to said first ingredient particles as substantially non-agglomerated individual particles, until at least about twenty percent by weight of the composite is said second ingredient.

### Claim 12 (depends on 11)

A method as set forth in claim 11, wherein said percentage is at least about 50.

### Claim 13 (depends on 11)

A method as set forth in claim 11, wherein said first ingredient comprises polypropylene or polyethylene.