Locked-wrap fuel rod
AssigneeThe United States of America as represented by the United States Energy Research and Development Administration
InventorsSamuel Kaplan, Alan J. Chertock, James R. Punches
Life of this patent
Estimating the term…
Abstract
A method for spacing fast reactor fuel rods using a wire wrapper improved by orienting the wire-wrapped fuel rods in a unique manner which introduces desirable performance characteristics not attainable by previous wire-wrapped designs. Use of this method in a liquid metal fast breeder reactor results in: (a) improved mechanical performance, (b) improved rod-to-rod contact, (c) reduced steel volume, and (d) improved thermal-hydraulic performance. The method produces a "locked wrap" design which tends to lock the rods together at each of the wire cluster locations.
Claims1
A method for wire-wrap spacing nuclear fuel rods for a fuel assembly containing a plurality of fuel rods in a triangular pitch array comprising the steps of:
- wrapping wire about each of the fuel rods in a helical pattern by using a wire of a diameter ranging from 0.035 to 0.053 inch such that a rod pitch to wire diameter ratio in the range of about 1.15 to about 1.30 can be maintained without wire-to-wire interference caused by overlapping of wires on adjacent fuel rods, and positioning the thus wrapped rods throughout the fuel assembly such that the groupings of three rods in any triangular pitch array will contain three different start positions of the wire wrapping by placing the groupings of three rods in 0.degree. -120.degree. -240.degree. orientations and such that the wire wrapping of adjacent rods forms a non-overlapping wire-to-wire contact forming a lock-wrap design tending to lock the rods together at each wire-wrap cluster.
Dependencies are inferred from the claim text.