# US 3,975,307 A · PTC thermistor composition and method of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 3,975,307 A
- Document ID: US3975307A
- Status: Granted
- Kind: A
- Application number: 05/513,474
- Filed: 1974-10-09
- Granted: 1976-08-17
- Earliest claimed: 1974-10-09
- Assignees: Matsushita Electric Industrial Co., Ltd.
- Inventors: Yoshihiro Matsuo; Masanori Fujimura; Tomizo Matsuoka; Shigeru Hayakawa
- Web page: https://patentgrep.com/patent/US3975307A

## CPC

- H01B 1/08: oxides
- H01C 1/1406: {Terminals or electrodes formed on resistive elements having positive temperature coefficient}
- H01C 7/025: {Perovskites, e.g. titanates}
- H05B 3/141: {Conductive ceramics, e.g. metal oxides, metal carbides, barium titanate, ferrites, zirconia, vitrous compounds}
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H01C: RESISTORS
- H05B: ELECTRIC HEATING; ELECTRIC LIGHT SOURCES NOT OTHERWISE PROVIDED FOR; CIRCUIT ARRANGEMENTS FOR ELECTRIC LIGHT SOURCES, IN GENERAL

## Abstract

A PTC thermistor composition comprising BaTiO.sub.3, TiO.sub.2, one oxide selected from the group consisting of Nb.sub.2 O.sub.5 and Y.sub.2 O.sub.3, Al.sub.2 O.sub.3, SiO.sub.2, Li.sub.2 CO.sub.3, MnO.sub.2 and one oxide selected from the group consisting of Sb.sub.2 O.sub.3 and Bi.sub.2 O.sub.3, and process for the production thereof are provided. Said process is characterized by the addition of TiO.sub.2 and Nb.sub.2 O.sub.5 to BaTiO.sub.3 before calcination and the addition of Al.sub.2 O.sub.3, SiO.sub.2, Li.sub.2 CO.sub.3, MnO.sub.2 and Sb.sub.2 O.sub.3 after the calcination. This PTC thermistor composition has a high breakdown voltage, a large electric current at the initial moment of a voltage application which current decreases rapidly with continuing voltage application, low specific resistivity and, good stability of resistivity.

## Claims

### Claim 1

A PTC thermistor composition comprising BaTiO.sub.3 as a major element and, as additive elements 0.05 to 1.24 percent by weight of SiO.sub.2, 0.007 to 0.09 percent by weight of a lithium compound convertible by air firing to lithium oxide, 0.003 to 0.04 percent by weight of MnO.sub.2 or manganese compound convertible by air firing to a manganese oxide, and 0.05 to 0.22 percent by weight of one oxide selected from the group consisting of Nb.sub.2 O.sub.5 and Y.sub.2 O.sub.3.

### Claim 2 (depends on 1)

A PTC thermistor composition according to claim 1, wherein said lithium compound is one member selected from the group consisting of Li.sub.2 CO.sub.3, LiNO.sub.3, Li.sub.2 SO.sub.4 and Li.sub.2 C.sub.2 O.sub.4.

### Claim 3 (depends on 1)

A PTC thermistor composition according to claim 1, wherein said manganese compound is one member selected from the group consisting of MnCO.sub.3, Mn(NO.sub.3).sub.2, and MnC.sub.2 O.sub.4.

### Claim 4 (depends on 1)

A PTC thermistor composition according to claim 1, which further comprises less than 1.30 percent by weight of TiO.sub.2.

### Claim 5 (depends on 4)

A PTC thermistor composition according to claim 4, which further comprises less than 1.26 percent by weight of Al.sub.2 O.sub.3.

### Claim 6 (depends on 5)

A PTC thermistor composition according to claim 5, which further comprises less than 0.12 percent by weight of one member selected from the group consisting of Sb.sub.2 O.sub.3 and Bi.sub.2 O.sub.3.

### Claim 7 (depends on 4)

A PTC thermistor composition according to claim 4, which further comprises less than 0.12 percent by weight of one member selected from the group consisting of Sb.sub.2 O.sub.3 and Bi.sub.2 O.sub.3.

### Claim 8 (depends on 1)

A PTC thermistor composition according to claim 1, which further comprises less then 1.26 percent by weight of Al.sub.2 O.sub.3.

### Claim 9 (depends on 8)

A PTC thermistor composition according to claim 8, which further comprises less than 0.12 percent by weight of Sb.sub.2 O.sub.3 and Bi.sub.2 O.sub.3.

### Claim 10 (depends on 1)

A PTC thermistor composition according to claim 1, which further comprises less than 0.12 percent by weight of Sb.sub.2 O.sub.3 and Bi.sub.2 O.sub.3.

### Claim 11 (depends on 1)

A PTC thermistor composition according to claim 1, wherein Ba in BaTiO.sub.3 is replaced by an amount of Sr less than 40 atomic percent.

### Claim 12 (depends on 1)

A PTC thermistor composition according to claim 1, wherein Ba in BaTiO.sub.3 is replaced by an amount of Pb less than 30 atomic percent.

### Claim 13 (depends on 1)

A PTC thermistor composition according to claim 1, wherein Ti in BaTiO.sub.3 is replaced by an amount of Sn less than 30 atomic percent.

### Claim 14 (depends on 1)

A PTC thermistor composition according to claim 1, wherein Ba in BaTiO.sub.3 is replaced by an amount of 1 to 30 atomic percent of Sr and by an amount 1 to 20 atomic percent of Pb.

### Claim 15 (depends on 1)

A PTC thermistor composition according to claim 1, wherein Ba in BaTiO.sub.3 is replaced by an amount of 1 to 20 atomic percent of Pb and Ti is replaced by an amount of 1 to 30 atomic percent of Sn.

### Claim 16

A method of producing a PTC thermistor comprising preparing a mixture consisting of BaCO.sub.3 and TiO.sub.2 to be converted into 99.89 to 95.73 percent by weight of BaTiO.sub.3, less than 1.30 percent by weight of TiO.sub.2 and 0.05 to 0.22 percent by weight of one oxide selected from the group consisting of Nb.sub.2 O.sub.5 and Y.sub.2 O.sub.3, calcining the mixture at a temperature of 900 to 1250.degree.C, milling the calcined material with additives of less than 1.26 percent by weight of Al.sub.2 O.sub.3, 0.05 to 1.24 percent by weight of SiO.sub.2, 0.007 to 0.09 percent by weight of Li.sub.2 CO.sub.3, 0.003 to 0.04 percent by weight of MnO.sub.2 and less than 0.12 percent by weight of one oxide selected from the group consisting of Sb.sub.2 O.sub.3 and Bi.sub.2 O.sub.3, pressing the mixture of the calcined material and said additives into a pressed body, firing the pressed body at a temperature of 1240.degree.C to 1400.degree.C for 0.5 to 5 hours, thereafter cooling the fired body to a temperature less than 800.degree.C at a cooling rate lower than 300.degree.C per hour, and thereafter cooling the thus cooled body to room temperature.