Method of reconstructing asphalt pavement
OwnerAngelo W. Benedettiinventor
Life of this patent
Estimating the term…
Abstract
The invention concerns heating an asphalt pavement in successive stages during time-spaced intervals. This permits the asphalt to be heated to its softening temperature without being overheated, and also permits the heat to penetrate deeply into the asphalt by conduction to soften the asphalt to a substantial depth (e.g. 1 inch or more). The asphalt is then scarified to a depth not greater than the depth to which it has been softened, and the scarified asphalt is then worked into a trafficable surface.
Claims14
A method of reconstructing asphalt pavement which comprises
- a. heating the surface of the pavement with radiant energy until a temperature at the pavement surface within the range of about 225.degree.F to about 325.degree.F is attained, thereby softening said surface;
- b. discontinuing the application of radiant energy;
- c. subjecting the structurally undisturbed pavement to a heat soaking step during which heat previously applied to the pavement surface is conducted into the interior of the pavement, the soaking interval being of sufficient duration to elevate the temperature of the interior of the pavement to at least the softening temperature of the asphalt;
- d. repeating steps (a) through (c) at least once, whereby the temperature of the interior of the pavement, to a depth of at least about one inch, is elevated to at least the softening temperature of the asphalt;
- e. scarifying the asphalt pavement to a depth not exceeding the depth to which the asphalt has been heated to at least its softening temperature, and
- f. providing said scarified asphalt pavement with a trafficable surface.
A continuous method of reconstructing asphalt pavement which comprises
- a. exposing the surface of the pavement to a radiant surface heated to a temperature within the range of about 1800.degree.F to about 2500.degree.F and continuing the exposure for a time sufficient to elevate the temperature of the surface of the pavement to a value within the range of from about 225.degree.F to about 325.degree.F, to thereby soften the pavement surface;
- b. discontinuing the exposure of the surface of the pavement to said radiant surface;
- c. subjecting the structurally undisturbed pavement to a heat soaking step during which heat previously applied to the pavement surface is conducted into the interior of the pavement, the soaking interval being of sufficient duration to elevate the temperature of the interior of the pavement to at least the softening temperature of the asphalt;
- d. repeating steps (a) through (c) at least once, whereby the temperature of the interior of the pavement, to a depth of at least about one inch, is elevated to at least the softening temperature of the asphalt;
- e. scarifying the asphalt pavement to a depth not exceeding the depth to which the asphalt has been heated to at least its softening temperature, and
- f. providing said scarified asphalt pavement with a trafficable surface.
A method of reconstructing asphalt pavement comprising
- a. heating the surface of the pavement until a temperature at the pavement surface of at least about 225.degree.F is attained, thereby softening said surface;
- b. discontinuing the application of heat;
- c. subjecting the structurally undisturbed pavement to a heat soaking step during which heat previously applied to the pavement surface is conducted into the interior of the pavement, the soaking interval being of sufficient duration to elevate the temperature of the interior of the pavement to at least the softening temperature of the asphalt;
- d. repeating steps (a) through (c) at least once, whereby the temperature of the interior of the pavement, to a depth of at least one half inch, is elevated to at least the softening temperature of the asphalt;
- e. scarifying the asphalt pavement to a depth not exceeding the depth to which the asphalt has been heated to at least its softening temperature, and
- f. providing said scarified asphalt pavement with a trafficable surface.
A method of reconstructing asphalt pavement comprising
- a. heating the surface of the pavement until a temperature at the pavement surface of at least about 225.degree.F is attained, thereby softening said surface;
- b. discontinuing the application of heat;
- c. subjecting the structurally undisturbed pavement to a heat soaking step during which heat previously applied to the pavement surface is conducted into the interior of the pavement, the soaking interval being of sufficient duration to elevate the temperature of the interior of the pavement to at least the softening temperature of the asphalt;
- d. repeating steps (a) through (c) at least once, whereby the temperature of the interior of the pavement, to an incremental depth, is elevated to at least the softening temperature of the asphalt;
- e. scarifying the asphalt pavement to a depth not exceeding the depth to which the asphalt has been heated to at least its softening temperature, and
- f. providing said scarified asphalt pavement with a trafficable surface.
Dependencies are inferred from the claim text.