Chromated copper arsenate wood preservative compositions
AssigneeKoppers Company, Inc.
InventorWilliam J. Oberley
Life of this patent
Estimating the term…
Abstract
Chromated copper arsentate wood preserving solutions in which the ratio of hexavalent chromium to trivalent chromium in the solution is between about 4.0:1.0 to about 1.0:1.0 give improved penetration into the wood, better retention of preservative in the wood, and improved stability of the treating solution. The solutions contain an acid to maintain the required pH, prevent corrosion, and further improve the solution stability.
Claims4
In a chromated copper arsenate wood treating solution of the type comprising as active ingredients from about 40.0 to about 70.0 % by weight chromium measured as CrO.sub.3, from about 15 to about 23 % by weight copper measured as CuO and from about 14.0 to about 50.0% by weight arsenic measured as As.sub.2 O.sub.5 ;
- the improvement comprising having in said solution trivalent chromium in a ratio of hexavalent chromium to trivalent chromium of from about 4.0:1.0 to about 1.0:1.0 and a pH below about 2.0.
In a method for treating wood with a chromated copper arsenate solution comprising impregnating the wood with a 1 to 10 percent by weight solution of a chromated copper arsenate composition;
- the improvement comprising having in said solution trivalent chromium in a ratio of hexavalent chromium to trivalent chromium of from about 4.0:1.0 to about 1.0:1.0.
Dependencies are inferred from the claim text.