Method of sealing a collation of battery layers together
AssigneeESB Incorporated
InventorsKent V. Anderson, John M. Bilhorn
Life of this patent
Estimating the term…
Abstract
The method, which provides liquid-impervious seals around opposed positive and negative battery electrodes in a collation of battery layers, concerns the need to apply energy around the opposed electrodes by some means other than and for a longer time period than the conventional pair of pressure rolls which have previously been used to seal moving battery layers. With this invention the seals are made by platens which either travel along with the moving collation during the sealing step or which are brought into contact with an increment of the collation which is temporarily stopped.
Claims5
The method of producing a seal around an increment of continuous, collated battery-layers,
- the collation including a layer having an increment on which there is a deposit of positive electrode,
- the collation also including a layer having an increment on which there is a deposit of negative electrode,
- the collation being further characterized as having the positive electrode substantially opposite the negative electrode,
- the method comprising the steps of:
- a. moving the collation of continuous battery layers;
- b. temporarily stopping the increment of the collation at a sealing station;
- c. moving an energy platen with respect to the stopped increment into a position so that the platen can transfer energy to the areas of the layers of the stopped increments surrounding the pair of opposed electrodes;
- and
- d. transferring energy from the platen to the layers in a manner, in an amount, and for a time sufficient to heat the areas of the layers surrounding the electrodes;
- e. subsequently maintaining pressure against the heated layers while simultaneously cooling the heated layers;
- f. removing the increment of the collation from the sealing station while the simultaneously advancing another increment of the collation to the sealing station;
- and,
- g. repeating steps (b), (c), (d), and (e) with respect to the other increment of the collation.
The method of sealing a collation of battery layers,
- the collation including a layer on which there is a deposit of positive electrode,
- the collation also including a layer on which there is a deposit of negative electrode,
- the collation being further characterized as having the positive electrode substantially opposite the negative electrode,
- the method comprising the steps of:
- a. moving the collation of battery layers;
- b. temporarily stopping the collation at a sealing station;
- c. moving an energy platen with respect to the stopped collation into a position so that the platen can transfer energy to the areas of the stopped collation to be sealed together;
- and,
- d. transferring energy from the platen to the layers in a manner, in an amount, and for a time sufficient to heat the areas of the layers surrounding the electrodes;
- e. subsequently maintaining pressure against the heated layers while simultaneously cooling the heated layers;
- f. removing the increment of the collation from the sealing station while simultaneously advancing another increment of the collation to the sealing station;
- and,
- g. repeating steps (b), (c), (d), and (e) with respect to the other increment of the collation.
Dependencies are inferred from the claim text.