Process for treating sewage sludge and fertilizer products thereof
AssigneeOrgonics, Inc.
InventorJames M. O'Donnell
Life of this patent
Estimating the term…
Abstract
An apparatus for and a process of treating sludge filter cake and the granular product thereof which comprises reducing the particle size and moisture content of the sludge cake, sterilizing the sludge cake by contacting the sludge cake with an N-methylol-urea solution, reacting the N-methylol-urea solution with the sludge cake at a pH of 3 to 5 while agitating the sludge particles to provide a granular-reaction product, and drying the product to provide a granular, high-nitrogen, odorless fertilizer or animal feed supplement product.
Claims21
A process for treating sludge filter cake material, which process comprises:
- a. reducing sludge filter cake material to a particle size of about 1/8th of an inch or less;
- b. reducing the moisture content of the reduced sludge particles to between about 30 and 50% to provide a partially dried sludge;
- c. introducing the sludge into a reactor and adding an acid to the partially dried sludge in the first section of the reactor to provide an acidic sludge having a pH of from about 3.0 to 5.0;
- d. providing an alkaline N-methylol-urea aqueous prepolymer solution wherein the methylol-urea is subject to condensation and comprises a mixture of mono and dimethylol urea, and wherein the prepolymer is prepared by the reaction of from about 1.1 to up to about 2.0 moles of urea per mole of formaldehyde in a reaction time of from about 10 to 30 minutes and at a temperature of from about 30.degree. to 80.degree.C;
- e. immediately reacting the prepolymer solution with the partially dried sludge in a second section of the reactor, the reaction carried out while continuously moving the sludge from the inlet to the outlet of the reactor, and at a temperature of from about 30.degree. to 80.degree.C and at a pH of from about 3 to 5, and while vigorously mixing the sludge particles in the first and second sections of the reactor for a time sufficient to complete the reaction and conversion of the prepolymer, and to provide a granular reaction product comprising the condensed polymer and dried sludge material, the condensed polymer having a molecular weight of less than about 300;
- and
- f. drying the reaction product at a temperature of less than 95.degree.C to a moisture content of about 3 to 10%, thereby providing a granular, high-nitrogen, odorless fertilizer or animal feed supplement product.
A process for treating sludge filter cake material, which process comprises in combination:
- a. shredding sludge filter cake material by conveying a moving bed of the material through a shredding means to provide a shredded sludge material of a particle size less than about 1/10th of an inch;
- b. preparing an N-methylol-urea aqueous prepolymer solution having a pH of from 7.0 to 8.5 and subject to condensation by the change in pH to 3.0 to 5.0, the prepolymer solution prepared by the reaction of from about 1.2 to 2.0 moles of urea per mole of formaldehyde in a reaction time of 10 to 30 minutes and at a temperature of about 30.degree. to 80.degree.C;
- c. introducing the shredded sludge material into the inlet of an elongated moving bed pug mill having a first and second section and containing a plurality of rotating paddles along its length for the vigorous agitation of the shredded material as it is moved from the inlet to the outlet of the pug mill;
- d. introducing an acid into the first section of the pug mill to maintain the pH of the shredded material at a pH of 3.0 to 5.0;
- e. introducing granular dry reaction product from the process into the first section of the pug mill in an amount sufficient, with the heat supplied to the pug mill and the heat of reaction, to reduce the moisture content of the shredded sludge material to less than 50%;
- f. spraying the prepolymer solution in the second section of the mill into the agitated acidic sludge material at a temperature of less than 80.degree.C and a pH of 3.0 to 5.0, and for a time sufficient to complete substantially the condensation and reaction of the prepolymer and to form a condensed polymeric reaction product;
- g. discharging a granular nitrogen-rich reaction product at a temperature of from about 50.degree. to 60.degree.C from the outlet of the pug mill;
- and
- h. drying the reaction product to a moisture content of between about 2 to 10% at a temperature of not more than 80.degree.C.
Dependencies are inferred from the claim text.