# US 2026/0314034 A1 · Method of forming semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0314034 A1
- Document ID: US20260314034A1
- Status: Published application
- Kind: A1
- Application number: 19/711,763
- Filed: 2026-06-17
- Published: 2026-10-08
- Earliest claimed: 2023-12-28
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Shao-Tse HUANG; Jin-Hao JHANG; Wei-De HO; Han-Yu LIN
- Web page: https://patentgrep.com/patent/US20260314034A1

## CPC

- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/0186: {Manufacturing their interconnections or electrodes, e.g. source or drain electrodes}
- H10D 84/0188: {Manufacturing their isolation regions}
- H10P 95/06: {Planarisation of inorganic insulating materials}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method includes a number of operations. A bottom transistor and a top transistor overlapping the bottom transistor are formed. A vertical local interconnect (VLI) structure is formed and electrically connects source/drain regions of the bottom transistor and the top transistor. A hard mask layer is formed over the VLI structure, wherein the hard mask layer includes a bottom nitride layer, a top nitride layer and an amorphous semiconductive layer directly between the bottom nitride layer and the top nitride layer. The hard mask layer is patterned. A trench is formed in the VLI structure. An isolation structure is formed in the trench. A first polishing process is performed to the isolation structure and the hard mask layer, wherein the first polishing process stops the amorphous semiconductive layer. A second polish process is performed to the isolation structure, the bottom nitride layer and the amorphous semiconductive layer.

## Claims

### Claim 1

A method comprising:
forming a lower transistor and an upper transistor over the lower transistor;
forming a vertical local interconnect (VLI) structure electrically connecting a source/drain region of the lower transistor to a source/drain region of the upper transistor;
forming a hard mask stack over the VLI structure, the hard mask stack comprising a first dielectric layer, a second dielectric layer and an amorphous semiconductor polish stop layer between the first dielectric layer and the second dielectric layer;
etching a portion of the VLI structure through the hard mask stack to form a recess in the VLI structure; and
forming an isolation structure in the recess.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
performing a first polishing process on the isolation structure and the hard mask stack, wherein the first polishing process stops at the amorphous semiconductor polish stop layer.

### Claim 3 (depends on 2)

The method of claim 2, further comprising:
after performing the first polishing process, performing a second polishing process on the isolation structure, the first dielectric layer, and the amorphous semiconductor polish stop layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first dielectric layer and the second dielectric layer comprise silicon nitride, and the amorphous semiconductor polish stop layer comprises amorphous silicon.

### Claim 5 (depends on 1)

The method of claim 1, wherein forming the hard mask stack further comprises forming an oxide layer over the second dielectric layer, wherein a thickness of the oxide layer is greater than a thickness of the second dielectric layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein etching the portion of the VLI structure comprises recessing the VLI structure such that a remaining portion of the VLI structure forms an L-shaped structure.

### Claim 7 (depends on 1)

The method of claim 1, wherein forming the isolation structure comprises:
forming a dielectric liner in the recess, wherein the dielectric liner laterally seals the amorphous semiconductor polish stop layer; and
forming a dielectric material over the dielectric liner to fill a remainder of the recess.

### Claim 8

A method comprising:
forming a lower transistor and an upper transistor over the lower transistor;
etching a first trench in gate electrodes of the lower and upper transistors;
forming an interconnect structure in the first trench;
forming a hard mask layer over the interconnect structure, wherein the hard mask layer comprises:
a first nitride layer over the interconnect structure;
a polish stop layer over the first nitride layer, wherein the first nitride layer is thinner than the polish stop layer; and
a second nitride layer over the polish stop layer;
patterning the hard mask layer;
etching a second trench based on the patterned hard mask layer; and
forming an isolation structure in the second trench.

### Claim 9 (depends on 8)

The method of claim 8, further comprising:
performing a first polishing process on the isolation structure and the hard mask layer, wherein the first polishing process stops at a level of the polish stop layer.

### Claim 10 (depends on 9)

The method of claim 9, further comprising:
after the first polishing process stops, performing a second polishing process on the isolation structure, the first nitride layer, and the polish stop layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein the first polishing process has a first polish selectivity between the second nitride layer and the polish stop layer, the second polishing process has a second polish selectivity between the first nitride layer and the polish stop layer, and the first polish selectivity is greater than the second polish selectivity.

### Claim 12 (depends on 8)

The method of claim 8, wherein the polish stop layer comprises amorphous silicon, and forming the isolation structure comprises forming an oxygen-free dielectric liner in the second trench.

### Claim 13 (depends on 8)

The method of claim 8, wherein forming the hard mask layer further comprises forming an oxide layer over the second nitride layer, and wherein a thickness of the oxide layer is greater than a thickness of any of the first nitride layer, the polish stop layer, and the second nitride layer.

### Claim 14 (depends on 8)

The method of claim 8, wherein etching the second trench comprises recessing the interconnect structure such that a remaining portion of the interconnect structure constitutes an L-shape.

### Claim 15

A method comprising:
forming a lower transistor and an upper transistor over the lower transistor;
forming a first trench in gate electrodes of the lower and upper transistors;
forming a dielectric liner in the first trench;
forming a conductive material in the first trench and over the dielectric liner;
forming a patterned hard mask layer over the dielectric liner and the conductive material;
forming a second trench in the conductive material by the patterned hard mask layer;
forming an insulation material in the second trench;
performing a first polishing process on the patterned hard mask layer and the insulation material, wherein the first polishing process stops at a first level higher than a top surface of the conductive material; and
after performing the first polishing process, performing a second polishing process on the patterned hard mask layer and excess portions of the insulation material higher than the top surface of the conductive material.

### Claim 16 (depends on 15)

The method of claim 15, wherein the patterned hard mask layer comprises a bottom mask layer, a top mask layer, and a polish stop layer directly between the bottom mask layer and the top mask layer, and wherein the first level corresponds to a level of the polish stop layer.

### Claim 17 (depends on 16)

The method of claim 16, wherein the bottom mask layer and the top mask layer comprise silicon nitride, and the polish stop layer comprises amorphous silicon.

### Claim 18 (depends on 16)

The method of claim 16, wherein the first polishing process polishes the top mask layer at a first polish rate and polishes the polish stop layer at a second polish rate, wherein the first polish rate is different from the second polish rate.

### Claim 19 (depends on 15)

The method of claim 15, wherein forming the insulation material comprises:
forming an oxygen-free liner in the second trench; and
forming an oxide material over the oxygen-free liner.

### Claim 20 (depends on 15)

The method of claim 15, wherein forming the second trench in the conductive material comprises etching a portion of the conductive material such that a remaining portion of the conductive material forms an L-shaped structure.