# US 2026/0308847 A1 · Single layer coated white kraftliner

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0308847 A1
- Document ID: US20260308847A1
- Status: Published application
- Kind: A1
- Application number: 19/171,085
- Filed: 2025-04-04
- Published: 2026-10-08
- Earliest claimed: 2025-04-04
- Applicants: Billerud Aktiebolag (publ)
- Inventors: Cassandra BOBART; James SHULTZ
- Web page: https://patentgrep.com/patent/US20260308847A1

## CPC

- D21H 11/04: Kraft or sulfate pulp
- D21H 19/385: {Oxides, hydroxides or carbonates}
- D21H 19/40: siliceous, e.g. clays
- D21H 19/54: Starch
- D21H 19/62: Macromolecular organic compounds or oligomers thereof obtained otherwise than by reactions only involving carbon-to-carbon unsaturated bonds
- D21H 19/84: on both sides of the substrate
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR

## Abstract

There is provided a single layer white kraftliner having a grammage from 100 to 220 g/m2 when measured according to ISO 536:2019, wherein the kraftliner: comprises bleached hardwood fibers and bleached softwood fibers in a dry weight ratio from 98:2 to 82:18; comprises a print surface and a back surface, the print surface being coated with a first coating composition comprising, by dry weight, 40-80 wt % clay, 10-45 wt % calcium carbonate and 5-25 wt % synthetic binder; has a specular gloss of more than 50% when measured at 75° according to ISO 8254-1:2009; has a Bendtsen roughness of less than 100 ml/min on at least one of the surfaces when measured according to ISO 8791-2:2013; and has a compressive strength index in the cross direction (CD) of at least 21 Nm/g when measured using a short-span compressive tester according to ISO 9895:2008. There is also provided a method of producing a single layer white kraftliner.

## Claims

### Claim 1

A single layer white kraftliner having a grammage from 100 to 220 g/m2 when measured according to ISO 536:2019, wherein the kraftliner:
comprises bleached hardwood fibers and bleached softwood fibers in a dry weight ratio from 98:2 to 82:18;
comprises a print surface and a back surface, the print surface being coated with a first coating composition comprising, by dry weight, 40-80 wt % clay, 10-45 wt % calcium carbonate and 5-25 wt % synthetic binder;
has a specular gloss of more than 50% when measured at 75° according to ISO 8254-1:2009;
has a Bendtsen roughness of less than 100 ml/min on at least one of the surfaces when measured according to ISO 8791-2:2013; and
has a compressive strength index in the cross direction (CD) of at least 21 Nm/g when measured using a short-span compressive tester according to ISO 9895:2008.

### Claim 2 (depends on 1)

The kraftliner of claim 1, which has a geometric tensile stiffness index of at least 5.2 kNm/g when measured according to ISO 1924-3:2005.

### Claim 3 (depends on 1)

The kraftliner of claim 1, which has a specific formation of less than 0.7 √g/m when measured according to SCAN-P 92:09.

### Claim 4 (depends on 1)

The kraftliner of claim 1, which has a specular gloss of at least 54% when measured at 75° according to ISO 8254-1:2009.

### Claim 5 (depends on 1)

The kraftliner of claim 1, which has brightness of at least 85% when measured according to ISO 2470-1:2016.

### Claim 6 (depends on 1)

The kraftliner of claim 1, which has a Bendtsen roughness of less than 60 ml/min on at least one of the surfaces when measured according to ISO 8791-2:2013.

### Claim 7 (depends on 1)

The kraftliner of claim 1, in which the first coating composition further comprises starch.

### Claim 8 (depends on 1)

The kraftliner of claim 1, in which the first coating composition comprises, by dry weight, 50-70 wt % clay, 13-35 wt % calcium carbonate and 7-20 wt % synthetic binder.

### Claim 9 (depends on 1)

The kraftliner of claim 1, in which the calcium carbonate in the first coating composition is a mixture of calcium carbonates comprising a calcium carbonate having a purity of ≤90% and a calcium carbonate having a purity of >90%.

### Claim 10 (depends on 9)

The kraftliner of claim 9, in which the dry weight ratio between the calcium carbonate having a purity of ≤90% and the calcium carbonate having a purity of >90% is within the range of 1:1 to 1:5.

### Claim 11 (depends on 1)

The kraftliner of claim 1, in which the back surface is coated with a second coating composition comprising starch and pigment.

### Claim 12 (depends on 11)

The kraftliner of claim 11, wherein the second coating composition further comprises synthetic binder.

### Claim 13 (depends on 11)

The kraftliner of claim 11, wherein the pigment in the second coating composition comprises clay pigment and/or calcium carbonate pigment.

### Claim 14 (depends on 11)

The kraftliner of claim 11, wherein the coat weight of the second coating composition is from 1 to 5 g/m2.

### Claim 15 (depends on 1)

The kraftliner of claim 1, wherein the coat weight of the first coating composition is from 6 to 18 g/m2.

### Claim 16 (depends on 1)

The kraftliner of claim 1, which has a density of 915-1100 kg/m3 when measured according to ISO 534:2011.

### Claim 17 (depends on 1)

The kraftliner of claim 1, which as a compressive strength index in the CD of at least 22 Nm/g when measured using a short-span compressive tester according to ISO 9895:2008.

### Claim 18

A method of producing a single layer white kraftliner comprising the steps of:
providing a furnish comprising bleached hardwood fibers and bleached softwood fibers in a dry weight ratio from 98:2 to 82:18;
forming a web from the furnish in a wire section comprising a headbox;
pressing the web from the wire section in a pressing section;
drying the web from the pressing section in a drying section to obtain a dried web;
calendering the dried web;
applying a first aqueous coating composition comprising, by dry weight, 40-80 wt % clay, 10-45 wt % calcium carbonate and 5-25 wt % synthetic binder to a print surface of the web to obtain a coated web; and
calendering the coated web.

### Claim 19 (depends on 18)

The method of claim 18, wherein the consistency of the furnish in the headbox is from 0.65% to 0.95%.

### Claim 20 (depends on 18)

The method of claim 18, wherein calcium carbonate is added to the furnish in an amount from 30 to 80 kg per ton of dry fiber.