# US 2026/0308829 A1 · Method for manufacturing fiber-resin composite material, method for manufacturing mobile phone case, and mobile phone case

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0308829 A1
- Document ID: US20260308829A1
- Status: Published application
- Kind: A1
- Application number: 19/679,778
- Filed: 2026-05-18
- Published: 2026-10-08
- Earliest claimed: 2023-11-16
- Assignees: Shenzhen Lingyi Innovation Technology Co., Ltd
- Applicants: Shenzhen Lingyi Innovation Technology Co., Ltd.
- Inventors: Jiali YU; Zhenhui YU; Yanghui ZHENG
- Web page: https://patentgrep.com/patent/US20260308829A1

## CPC

- D06B 5/22: through fabrics
- D06M 15/564: Polyureas, polyurethanes or other polymers having ureide or urethane links; Precondensation products forming them
- D06M 2101/36: Aromatic polyamides
- D10B 2331/021: aromatic polyamides, e.g. aramides
- D06B: TREATING TEXTILE MATERIALS USING LIQUIDS, GASES OR VAPOURS (mechanical treatment of natural fibrous or filamentary material to obtain fibres or filaments D01B)
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

A method for manufacturing a fiber-resin composite material includes: obtaining an aramid fiber woven fabric having a grammage of 100 g/m2 to 350 g/m2 and having N stacked layers, as a base material, where the N is a positive integer greater than or equal to 1; obtaining a resin having a Shore hardness of 30 A and 85D as a composite layer, and performing full or semi-pre-impregnation on the composite layer and the base material, so as to obtain a semi-finished fiber-resin composite material; performing hot pressing on the semi-finished fiber-resin composite material, where a hot pressing temperature is 150° C. to 250° C., a hot pressing pressure is 40 bar to 55 bar, and a hot pressing duration is 2 min to 10 min; after performing the hot pressing for a preset hot pressing duration, stopping heating the semi-finished fiber-resin composite material, so as to obtain a fiber-resin composite material.

## Claims

### Claim 1

A method for manufacturing a fiber-resin composite material, comprising:
obtaining an aramid fiber woven fabric as a base material, wherein the aramid fiber woven fabric has a grammage in a range of 100 g/m2 to 350 g/m2, and the aramid fiber woven fabric has N stacked layers, the N is a positive integer greater than or equal to 1;
obtaining a resin having a Shore hardness in a range of 30 A to 85 D as a composite layer, and performing full pre-impregnation or semi-pre-impregnation on the composite layer and the base material, so as to obtain a semi-finished fiber-resin composite material;
placing the semi-finished fiber-resin composite material in a hot pressing device for hot pressing, enabling the resin to penetrate into gaps of the aramid fiber woven fabric, wherein a temperature of the hot pressing in the hot pressing device is in a range of 150° C. to 250° C., a pressure of the hot pressing is in a range of 40 bar to 55 bar, and a duration of the hot pressing is in a range of 2 min to 10 min;
after the hot pressing performed on the semi-finished fiber-resin composite material for a preset hot pressing duration, stopping heating the semi-finished fiber-resin composite material, so as to obtain a finished fiber-resin composite material.

### Claim 2 (depends on 1)

The method according to claim 1, wherein, a value of the Nis negatively correlated with the grammage of the aramid fiber woven fabric, and 1≤N≤5.

### Claim 3 (depends on 2)

The method according to claim 2, wherein,
the aramid fiber woven fabric has a grammage of 300±50 g/m2, the aramid fiber woven fabric has 1 layer to 3 stacked layers, and the composite layer is a resin having a Shore hardness in a range of 80 A to 50 D.

### Claim 4 (depends on 2)

The method according to claim 2, wherein,
the aramid fiber woven fabric has a grammage of 150±15 g/m2, the aramid fiber woven fabric has 3 stacked layers to 5 stacked layers, and the composite layer is a resin having a Shore hardness of 90 A to 65 D.

### Claim 5 (depends on 1)

The method according to claim 1, wherein, the composite layer is a resin having a Shore hardness of 80 A to 80 D; and for the finished fiber-resin composite material, a thickness of each of the N stacked layers is in a range of 0.15 mm to 1 mm.

### Claim 6 (depends on 1)

The method according to claim 1, wherein, the obtaining the resin having the Shore hardness in the range of 30 A to 85 D as a composite layer and performing semi-pre-impregnation on the composite layer and the base material, so as to obtain the semi-finished fiber-resin composite material, comprises:
obtaining a resin having a Shore hardness in a range of 30 A to 85 D as the composite layer, and stacking the composite layer with the aramid fiber woven fabric;
performing semi-pre-impregnation, using a hot pressing roller, on the stacked composite layer and aramid fiber woven fabric, so as to obtain the semi-finished fiber-resin composite material.

### Claim 7 (depends on 1)

The method according to claim 1, wherein, the obtaining the resin having the Shore hardness in the range of 30 A to 85 D as a composite layer and performing full pre-impregnation on the composite layer and the base material, so as to obtain the semi-finished fiber-resin composite material, comprises:
obtaining a resin having a Shore hardness in a range of 30 A to 85 D as the composite layer, melting the composite layer and placing the melted composite layer in a pre-impregnation apparatus; and
placing the aramid fiber woven fabric in the pre-impregnation apparatus for full pre-impregnation, so as to obtain the semi-finished fiber-resin composite material.

### Claim 8

A method for manufacturing a mobile phone case, comprising:
obtaining a fiber-resin composite material as a first sheet material;
cutting the first sheet material to obtain a preset sheet material in a preset size and in a preset shape, wherein, the preset sheet material comprises a central region and an edge region surrounding the central region;
obtaining a semi-cured material or a cured material as a second sheet material, attaching the second sheet material to the central region of the preset sheet material, and placing the second sheet material together with the preset sheet material into a mobile phone case mold;
performing secondary molding on the second sheet material and the preset sheet material, wherein a temperature of the secondary molding is in a range of 160° C. to 200° C., a pressure of the secondary molding is in a range of 35 bar to 45 bar, and a duration of the secondary molding is in a range of 5 min to 15 min;
after the duration of the secondary molding performed on the second sheet material and the preset sheet material reaching a preset molding duration, cooling the second sheet material and the preset sheet material to a room temperature, so as to obtain a finished mobile phone case;
wherein, the fiber-resin composite material is manufactured by:
obtaining an aramid fiber woven fabric as a base material, wherein the aramid fiber woven fabric has a grammage in a range of 100 g/m2 to 350 g/m2, and the aramid fiber woven fabric has N stacked layers, the N is a positive integer greater than or equal to 1;
obtaining a resin having a Shore hardness in a range of 30 A to 85 D as a composite layer, and performing full pre-impregnation or semi-pre-impregnation on the composite layer and the base material, so as to obtain a semi-finished fiber-resin composite material;
placing the semi-finished fiber-resin composite material in a hot pressing device for hot pressing, enabling the resin to penetrate into gaps of the aramid fiber woven fabric, wherein a temperature of the hot pressing in the hot pressing device is in a range of 150° C. to 250° C., a pressure of the hot pressing is in a range of 40 bar to 55 bar, and a duration of the hot pressing is in a range of 2 min to 10 min;
after the hot pressing performed on the semi-finished fiber-resin composite material for a preset hot pressing duration, stopping heating the semi-finished fiber-resin composite material, so as to obtain a fiber-resin composite material.

### Claim 9 (depends on 8)

The method according to claim 8, wherein, a value of the N is negatively correlated with the grammage of the aramid fiber woven fabric, and 1≤N≤5.

### Claim 10 (depends on 9)

The method according to claim 9, wherein,
the aramid fiber woven fabric has a grammage of 300±50 g/m2, the aramid fiber woven fabric has 1 layer to 3 stacked layers, and the composite layer is a resin having a Shore hardness in a range of 80 A to 50 D.

### Claim 11 (depends on 9)

The method according to claim 9, wherein,
the aramid fiber woven fabric has a grammage of 150±15 g/m2, the aramid fiber woven fabric has 3 stacked layers to 5 stacked layers, and the composite layer is a resin having a Shore hardness of 90 A to 65 D.

### Claim 12 (depends on 8)

The method according to claim 8, wherein, the obtaining the resin having the Shore hardness in the range of 30 A to 85 D as the composite layer, and performing semi-pre-impregnation on the composite layer and the base material, so as to obtain the semi-finished fiber-resin composite material, comprises:
obtaining a resin having a Shore hardness in a range of 30 A to 85 D as the composite layer, and stacking the composite layer with the aramid fiber woven fabric;
performing semi-pre-impregnation, using a hot pressing roller, on the stacked composite layer and aramid fiber woven fabric, so as to obtain the semi-finished fiber-resin composite material.

### Claim 13 (depends on 8)

The method according to claim 8, wherein, the obtaining the resin having the Shore hardness in the range of 30 A to 85 D as the composite layer, and performing full pre-impregnation on the composite layer and the base material, so as to obtain the semi-finished fiber-resin composite material, comprises:
obtaining a resin having a Shore hardness in a range of 30 A to 85 D as the composite layer, melting the composite layer and placing the melted composite layer in a pre-impregnation apparatus; and
placing the aramid fiber woven fabric in the pre-impregnation apparatus for full pre-impregnation, so as to obtain the semi-finished fiber-resin composite material.

### Claim 14 (depends on 8)

The method according to claim 8, wherein,
the second sheet material is formed of the semi-cured material, and the second sheet material is a fiberglass board.

### Claim 15 (depends on 8)

The method according to claim 8, wherein the second sheet material is formed of the cured material, and the second sheet material is a carbon fiber board, a stainless steel board, or a PC board.

### Claim 16

A mobile phone case, comprising: a body portion made of a fiber-resin composite material and a reinforcing portion made of a semi-cured material or a cured material,
wherein, the body portion comprises a carrying portion for contacting a rear of a phone and a wrapping portion for wrapping sides of the phone; the reinforcing portion is disposed on the carrying portion; the fiber-resin composite material comprises an aramid fiber woven fabric layer and a resin composite layer; the aramid fiber woven fabric layer comprises 1 layer to 5 stacked layers of aramid fiber woven fabric, the aramid fiber woven fabric layer has a grammage in a range of 100 g/m2 to 350 g/m2, and the resin composite layer has a Shore hardness in a range of 80 A to 80 D.

### Claim 17 (depends on 16)

The mobile phone case according to claim 16, wherein,
the aramid fiber woven fabric layer comprises 1 layer to 3 stacked layers of aramid fiber woven fabric, the aramid fiber woven fabric layer has a grammage of 300±50 g/m2, and the resin composite layer has a Shore hardness of 80 A to 50 D.

### Claim 18 (depends on 16)

The mobile phone case according to claim 16, wherein,
the aramid fiber woven fabric layer comprises 3 stacked layers to 5 stacked layers of aramid fiber woven fabric, the aramid fiber woven fabric layer has a grammage of 150±15 g/m2, and the resin composite layer has a Shore hardness of 90 A to 65 D.

### Claim 19 (depends on 16)

The mobile phone case according to claim 16, wherein,
the resin composite layer is TPE resin or TPU resin; the reinforcing portion is formed of the semi-cured material, and the semi-cured material is a fiberglass board.

### Claim 20 (depends on 16)

The mobile phone case according to claim 16, wherein,
the reinforcing portion is formed of the cured material, and the cured material is a carbon fiber board, a stainless steel board, or a PC board.