# US 2026/0308811 A1 · High-temperature-resistant wear-resistant brush material and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0308811 A1
- Document ID: US20260308811A1
- Status: Published application
- Kind: A1
- Application number: 19/479,957
- Filed: 2024-11-04
- Published: 2026-10-08
- Earliest claimed: 2023-11-07
- Applicants: Guangzhou Aoqun New Materials Co., Ltd.
- Inventors: Xuezhen LIU; Min WANG; Zhiqiang LIU
- Web page: https://patentgrep.com/patent/US20260308811A1

## CPC

- D01F 1/103: {Agents inhibiting growth of microorganisms}
- D01D 1/106: {Filtering}
- D01D 10/02: Heat treatment (heating for finishing D02J13/00)
- D01D 10/06: Washing or drying
- D01F 8/12: with at least one polyamide as constituent
- D01F 8/14: with at least one polyester as constituent
- D01F 8/18: from other substances
- D10B 2401/13: anti-allergenic or anti-bacterial
- D10B 2503/00: Domestic or personal
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

Provided are a high-temperature-resistant wear-resistant brush material and a preparation method thereof. The preparation method includes: mixing an epoxy resin, polyacrylamide and polycaprolactone, conducting a heat treatment and crushing, dispersing an obtained powder in a tetrahydrofuran aqueous solution, adding an anhydride compound and uniformly mixing, conducting a reaction under ultraviolet irradiation while stirring, and conducting vacuum freeze drying after the reaction is finished, to obtain a product A; mixing a rare earth metal, iron and a quicklime, pretreating, calcining, dissolving a resulting calcined product in an organic alcohol solution after the reaction is finished, adding nanoparticles, uniformly stirring, maintaining a temperature, and then filtering, washing and drying to obtain a product B; and mixing the product A, the product B and an auxiliary agent, uniformly stirring in a kneader, and finally drawing to obtain the high-temperature-resistant wear-resistant brush material.

## Claims

### Claim 1

A method for preparing a drawing raw material, the method comprising the following steps:
mixing an epoxy resin, polyacrylamide and polycaprolactone, and treating at a temperature of 60° C. to 80° C. for 1 hour to 3 hours, cooling an obtained product to room temperature and crushing to 80 mesh to 200 mesh, dispersing an obtained powder in a tetrahydrofuran aqueous solution with a concentration of 10% to 20%, adding an anhydride compound to an obtained solution and mixing, subjecting a resulting mixture to a reaction under ultraviolet (UV) irradiation while stirring, and after the reaction is finished, subjecting a resulting reaction product to vacuum freeze drying to obtain a product A, wherein a mass ratio of the epoxy resin, the polyacrylamide, the polycaprolactone, and the anhydride compound is in a range of 1:1-3:0.2-0.7:0.07-0.09;
mixing a rare earth metal, iron and a quicklime, pretreating at a temperature of 200° C. to 400° C. for 1 hour to 3 hours, then heating to a temperature of 1200° C. to 1400° C. and calcining for 2 hours to 4 hours, dissolving a resulting calcined product in an organic alcohol solution after the calcining is finished, adding nanoparticles, stirring, and treating at a temperature of 40° C. to 60° C. for 24 hours to 48 hours while maintaining the temperature, and then filtering, washing and drying to obtain a product B, wherein a mass ratio of the rare earth metal, the iron, the quicklime and the nanoparticles is in a range of 1:3-6:10-15:100; and
mixing the product A, the product B and an auxiliary agent in a mass ratio of 1:0.01-0.05:0.03-0.07, and then stirring in a kneader to obtain the drawing raw material.

### Claim 2 (depends on 1)

The method of claim 1, wherein the epoxy resin has a weight average molecular weight of 20,000 to 60,000, the polyacrylamide has a weight average molecular weight of 10,000 to 80,000, and the polycaprolactone has a weight average molecular weight of 10,000 to 50,000.

### Claim 3 (depends on 1)

The method of claim 1, wherein the anhydride compound is at least one selected from the group consisting of maleic anhydride, cyclopentene-1,2-dicarboxylic anhydride, 1,4-cyclohexadiene-1,2-dicarboxylic anhydride, N-allylisatoic anhydride, bicyclo(2.2.2)oct-5-ene-2,3-dicarboxylic anhydride, 2,3-dimethylmaleic anhydride and norbornene dianhydride.

### Claim 4 (depends on 1)

The method of claim 1, wherein the reaction under the ultraviolet irradiation is conducted under the following conditions: a power of an ultraviolet lamp being 150 W to 200 W, a main wavelength range of the ultraviolet lamp being 250 nm to 400 nm, an irradiation distance being 10 cm to 20 cm, an irradiation intensity being 1.0 mW/cm to 2.0 mW/cm and an irradiation time being 4 hours to 10 hours.

### Claim 5 (depends on 1)

The method of claim 1, wherein the rare earth metal is at least one selected from the group consisting of scandium, yttrium, lanthanum, cerium, praseodymium, neodymium, promethium, samarium, europium, gadolinium, terbium, dysprosium, holmium, erbium, thulium, ytterbium, and lutetium.

### Claim 6 (depends on 1)

The method of claim 1, wherein the organic alcohol is at least one selected from the group consisting of methanol, ethanol, ethylene glycol, and glycerol.

### Claim 7 (depends on 1)

The method of claim 1, wherein the nanoparticles are at least one selected from the group consisting of nano-aluminum trioxide, nano-aluminum nitride, nano-titanium dioxide, nano-shell powder, nano graphene and nano montmorillonite.

### Claim 8 (depends on 1)

The method of claim 1, wherein the auxiliary agent is a mixture consisting of a wetting agent, an antioxidant, and an accelerator in a mass ratio of 1:1:0.1-0.5;
the wetting agent is at least one selected from the group consisting of poly-N-vinylpyrrolidone, poly-N-vinyl-2-piperidone, poly-N-vinyl-3-methyl-2-piperidone, poly-N-vinyl-4-methyl-2-piperidone, poly-N-vinyl-3-ethyl-2-pyrrolidone, and poly-N-vinyl-4,5-dimethyl-2-pyrrolidone;
the antioxidant is one selected from the group consisting of pentaerythritol tetrakis[β-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate], and tris(2,4-tert-butylphenyl)phosphite; and
the accelerator is one selected from the group consisting of 2-mercaptobenzothiazole, dibenzothiazole disulfide, and N-cyclohexyl-2-benzothiazole sulfenamide and tetramethylthiuram disulfide.

### Claim 9 (depends on 1)

The method of claim 1, wherein the epoxy resin is a bisphenol A epoxy resin.

### Claim 10 (depends on 1)

The method of claim 1, wherein a mass ratio of the epoxy resin, the polyacrylamide, the polycaprolactone, and maleic anhydride is 1:2:0.45:0.08, 1:3:0.2:0.07, 1:1:0.2:0.09 or 1:1:0.7:0.09.

### Claim 11 (depends on 1)

The method of claim 1, wherein the mass ratio of the rare earth metal, the iron, the quicklime and the nanoparticles is 1:4.5:13:100, 1:3:15:100, 1:4:12:100 or 1:6:10:100.

### Claim 12 (depends on 1)

The method of claim 1, wherein the mass ratio of the product A, the product B and the auxiliary agent is 1:0.04:0.05, 1:0.01:0.07, 1:0.02:0.06 or 1:0.05:0.03.

### Claim 13 (depends on 8)

The method of claim 8, wherein the auxiliary agent is a mixture consisting of the wetting agent, the antioxidant, and the accelerator in the mass ratio of 1:1:0.1, 1:1:0.4 or 1:1:0.5.

### Claim 14 (depends on 1)

A drawing raw material prepared by the method of claim 1, wherein the drawing raw material comprises the product A, the product B and the auxiliary agent; and the mass ratio of the product A, the product B and the auxiliary agent is in a range of 1:0.01-0.05:0.03-0.07.

### Claim 15 (depends on 14)

A preparation method of a wear-resistant brush material, comprising the following steps: drawing the drawing raw material of claim 14 using a drawing machine equipped with a thermostatic device, to obtain the wear-resistant brush material after the drawing is finished.

### Claim 16 (depends on 15)

The preparation method of claim 15, wherein operating conditions of the drawing machine comprise: a drawing speed being 0.1 m/s to 0.5 m/s, and a drawing temperature being 250° C. to 300° C.

### Claim 17 (depends on 16)

A wear-resistant brush material prepared by the preparation method of claim 16.

### Claim 18

(canceled)

### Claim 19 (depends on 2)

The method of claim 2, wherein the epoxy resin is a bisphenol A epoxy resin.

### Claim 20 (depends on 12)

The method of claim 12, wherein the auxiliary agent is a mixture consisting of the wetting agent, the antioxidant, and the accelerator in the mass ratio of 1:1:0.1, 1:1:0.4 or 1:1:0.5.